Haysite H1000 Polyester Laminate

Category Polymer , Thermoset , Polyester, TS , Thermoset Polyester Glass SMC
Manufacturer Haysite
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Haysite H1000 Polyester Laminate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Haysite Grade 1000 laminate sheet is an outstanding material that is used in applications requiring exceptional weather and corrosion resistance. Grade H1000's unique polyester resin system provides corrosion resistance in sunlight and harsh weather environments in addition to meeting NEMA GPO-3 specifications for track resistance, flame retardance, heat resistance and physical properties. H1000 is particularly qualified for applications in the transportation industry due to its' low smoke generation, low smoke toxicity & halogen-free flame retardants. H1000 meets the rigid New York City Transit - Specification #64. Transit Authorities use Grade H1000 under their 3rd rail ties to provide electrical insulation, corrosion protection, UV resistance & most importantly to insure low smoke/flame toxicity in case of electrical failure. H1000, in a pultruded profile shape is used for electrical insulation for electrical cables, conduit & 3rd rail protection for workers.Information provided by Haysite
Physical Properties Metric English Comments
Water Absorption 0.16 %
0.16 %
ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength 89.6 MPa
13000 psi
CW; ASTM D638
93.1 MPa
13500 psi
LW; ASTM D638
Tensile Modulus 11.4 GPa
1650 ksi
LW; ASTM D638
11.4 GPa
1650 ksi
CW; ASTM D638
Flexural Strength 155 MPa
22500 psi
CW; ASTM D790
178 MPa
25800 psi
LW; ASTM D790
Flexural Modulus 9.17 GPa
1330 ksi
CW; ASTM D790
13.0 GPa
1880 ksi
LW; ASTM D790
Compressive Strength 207 MPa
30000 psi
Flatwise; ASTM D695
Izod Impact, Notched 5.55 J/cm
10.4 ft-lb/in
CW; ASTM D257
6.41 J/cm
12.0 ft-lb/in
LW; ASTM D256
Thermal Properties Metric English Comments
CTE, linear 12.6 µm/m-°C
7.00 µin/in-°F
ASTM D696
Flammability, UL94 V-0
V-0
Flame Spread Index 20
20
ASTM E84
Smoke Density 4.0 min
4.0 min
6.3 Optical Density; ASTM E661
Electrical Properties Metric English Comments
Dielectric Strength 11.4 kV/mm
290 kV/in
Perpendicular; ASTM D149
Arc Resistance 193 sec
193 sec
ASTM D495
Track Resistance >= 11 sec

@Thickness 6.35 mm
>= 11 sec

@Thickness 0.250 in
ASTM D2303
Descriptive Properties Value Comments
Flame Resistance 35 seconds
Burning Time, ASTM D229
80 seconds
Ignition Time, ASTM D229
Radiant Panel 15.9
ASTM E162
Smoke and Toxicity Data Aldehydes
10 ppm, BSS7239
Carbon Dioxide
2400 ppm, BSS7239
Carbon Monoxide
700 ppm, BSS7239
Hydrogen Bromide
0.5 ppm, BSS7239
Oxides of Nitrogen
4.5 ppm, BSS7239
Smoke Developed Index
165, ASTM E84