Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ACC Magnifoam™ MFSILTEC™ Roll Stock MTI Silicones Silicone Foam

Category Polymer , Thermoset , Silicone , Silicone Foam
Manufacturer Amber Chemical Company
Trade Name Magnifoam™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ACC Magnifoam™ MFSILTEC™ Roll Stock MTI Silicones Silicone Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Part of the Amber Chemical Group. Data provided by manufacturer.
Physical Properties Metric English Comments
Density 0.192 g/cc
0.00694 lb/in³
ASTM D1056
Water Absorption 3.0 %
3.0 %
ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Yield 0.207 MPa
30.0 psi
ASTM D412
Elongation at Break 100 %
100 %
ASTM D412
Compressive Strength 0.0276 MPa
4.00 psi
0.25; ASTM D3675
Compression Set 2.0 %
2.0 %
at 50%, 22 hrs @ 70°C; ASTM D1056
<= 10 %

@Temperature 100 °C
<= 10 %

@Temperature 212 °F
at 50%, 22 hrs; ASTM D1056
Thermal Properties Metric English Comments
Flammability, UL94 V-1
V-1
Rating dependent on color and thickness
V-0
V-0
Rating dependent on color and thickness
Flammability Test <= 25
<= 25
ASTM E162/D 3675
Smoke Density 1.5 min
1.5 min
<20; ASTM E662
4.0 min
4.0 min
<50; ASTM E662
Descriptive Properties Value Comments
Thermal Resistance, ft2-h/BTU 2.5
ASTM C518
Toxic Gas Emission Pass
Bombardier SMP 800C
Vertical Flammability Pass
FAR25.83(a)(1)(i) 12sec
Pass
FAR25.83(a)(1)(i) 60sec
Users viewing this material also viewed the following: