Thermal Properties Metric English Comments
Flash Point 27.0 - 32.0 °C
80.6 - 89.6 °F
LG Chemical M-Xylene
Aromatic liquid similar to DIESELStructure & Characteristics: C6H4(CH3)2. Synthesized by extraction (using solvent) followed by purification of pyrolysis gasoline evolved from NCC process. Has 3 iso..
Flash Point 27.0 - 32.0 °C
80.6 - 89.6 °F
LG Chemical O-Xylene
Aromatic liquid similar to DIESELStructure & Characteristics: C6H4(CH3)2. Synthesized by extraction (using solvent) followed by purification of pyrolysis gasoline evolved from NCC process. Has 3 iso..
Flash Point 27.0 - 32.0 °C
80.6 - 89.6 °F
LG Chemical P-Xylene
Aromatic liquid similar to DIESELStructure & Characteristics: C6H4(CH3)2. Synthesized by extraction (using solvent) followed by purification of pyrolysis gasoline evolved from NCC process. Has 3 iso..
Flash Point 27.0 °C
80.6 °F
ASTM D3278, Seta Flash, Closed Cup
Lord Adhesives Chemglaze® V004 Polyurethane Coating
Chemglaze® V-Line polyurethane coatings are moisture curing aliphatic polyurethane coatings. They are used in product finishing applications on polyvinyl-chloride (PVC) and other plastics where m..
Flash Point 27.0 °C
80.6 °F
7204 Cross-linker; Seta
Lord Adhesives Flocklok® 7000/7204 Flock Adhesive
LORD Flocklok® 7000/7204 adhesive is a two-part, single-coat adhesive used for adhering polyester or nylon flock fibers to a variety of thermoplastics, including PVC, Alcryn®, Sunprene®, ny..
Flash Point 27.0 °C
80.6 °F
closed cup
Dow Corning 805 RESIN
Silicone binder resin for maintenance paints, colored baking enamels, decorative finishes; primarily with metallic pigments. Used alone or blended with Dow Corning® 806A Resin to promote intermedia..
Flash Point 27.0 °C
80.6 °F
closed cup
Dow Corning 808 RESIN
Medium-soft, silicone resin binder for heat resistant maintenance paints and colored baking enamels.Information provided by Dow Corning
Flash Point 27.0 °C
80.6 °F
closed cup
Dow Corning HV 1860/120 PRIMER
Primer designed for use with peroxide curing silicone rubbers to provide good bonding to metal, glass fibre and epoxy resinInformation provided by Dow Corning
Flash Point 27.0 °C
80.6 °F
closed cup
Dow Corning Q2-7406 ADHESIVE
Dow Corning® Q2-7406 Adhesive is a polydimethylsiloxane gum and resin dispersion; provides excellent high temperature properties with adhesion to 288C (550F).Information provided by Dow Corning
Flash Point 27.0 °C
80.6 °F
closed cup
Dow Corning Q2-7566 ADHESIVE
Dow Corning® Q2-7566 Adhesive is a high viscosity, polydimethylsiloxane gum and resin dispersion, providing excellent high temperature properties with adhesion to 288C (550F).Information provided b..
Flash Point 27.0 °C
80.6 °F
closed cup
Dow Corning Q2-7735 ADHESIVE
Dow Corning® Q2-7735 Adhesive is a polydimethylsiloxane gum and resin dispersion, and provides high tack combined with good adhesion.Information provided by Dow Corning
Flash Point >= 27.0 °C
>= 80.6 °F
closed cup
Dow Corning SYL-OFF® 23A CATALYST
Liquid. Standard cure. A 50% solids dispersion of an organotin complex in xylene.Information provided by Dow Corning
Flash Point 27.0 °C
80.6 °F
closed cup
Dow Corning SYL-OFF® C4-2109 RELEASE ADDITIVE
C4-2109 is a 10% active solids solution of a silicate based compound. This product is recommended for use as a release modifier for Syl-Off® brand solvent based, condensation curing, systems.Inform..
Flash Point 27.0 °C
80.6 °F
closed cup
Dow Corning Z-6264 SILANE
Dow Corning® Z-6264 Silane is an alkylalkoxysilane. It has an n-propyl organic group and a trimethoxysilyl inorganic group.Information provided by Dow Corning
Flash Point 27.0 °C
80.6 °F
closed cup
Dow Corning 1-6184 WATER REPELLENT
Dow Corning® 1-6184 Water Repellent is a low-VOC, multifunctional, self-crosslinking, water soluble siloxaneInformation provided by Dow Corning
Flash Point 27.0 °C
80.6 °F
Dow Corning 1250 SURFACTANT
50% silicone resin in Xylene solvent. Silicone Profoamer for mechanically frothing PVC dispersions. Good foam control for PVC foam coatings. Better water resistance and less odor than alkali metal s..
Flash Point 27.0 °C
80.6 °F
closed cup
Dow Corning 409 HS RESIN
High-performance coatings; high-temperature applications where low VOC content is required. Used alone or blended with a variety of solvent-based silicone and organic resins. Similar to Dow Corning®..
Flash Point 27.0 °C
80.6 °F
BASF 3-Methoxypropylamine (MOPA)
Formula: C4H11NOCAS: 5332-73-0Description: 3-Methoxypropylamine (MOPA) is a colorless to yellow liquid with an aminelike odor. It is miscible in water.Synonyms: 3-Aminopropyl methyl ether, 3-Methox..
Flash Point 27.0 °C
80.6 °F
BASF Cyclopentanone
Formula: C5H8OCAS: 120-92-3Description: Cyclopentanone is a water-white liquid, soluble in water, alcohol and ether.Applications: Intermediate used in the production of pharmaceuticals, biologicals,..
Flash Point 27.0 °C
80.6 °F
BASF Cyclohexylamine (CHA)
Formula: C6H13NCAS: 108-91-8Description: Cyclohexylamine i(CHA) s a colorless to yellow liquid with an amine-like odor. It is miscible with water.Synonyms: CHA, Cyclohexylamine, Cyclohexyl amine, 1-..