Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 27.0 - 32.0 °C | 80.6 - 89.6 °F | |
LG Chemical M-Xylene Aromatic liquid similar to DIESELStructure & Characteristics: C6H4(CH3)2. Synthesized by extraction (using solvent) followed by purification of pyrolysis gasoline evolved from NCC process. Has 3 iso.. |
|||
Flash Point | 27.0 - 32.0 °C | 80.6 - 89.6 °F | |
LG Chemical O-Xylene Aromatic liquid similar to DIESELStructure & Characteristics: C6H4(CH3)2. Synthesized by extraction (using solvent) followed by purification of pyrolysis gasoline evolved from NCC process. Has 3 iso.. |
|||
Flash Point | 27.0 - 32.0 °C | 80.6 - 89.6 °F | |
LG Chemical P-Xylene Aromatic liquid similar to DIESELStructure & Characteristics: C6H4(CH3)2. Synthesized by extraction (using solvent) followed by purification of pyrolysis gasoline evolved from NCC process. Has 3 iso.. |
|||
Flash Point | 27.0 °C | 80.6 °F | ASTM D3278, Seta Flash, Closed Cup |
Lord Adhesives Chemglaze® V004 Polyurethane Coating Chemglaze® V-Line polyurethane coatings are moisture curing aliphatic polyurethane coatings. They are used in product finishing applications on polyvinyl-chloride (PVC) and other plastics where m.. |
|||
Flash Point | 27.0 °C | 80.6 °F | 7204 Cross-linker; Seta |
Lord Adhesives Flocklok® 7000/7204 Flock Adhesive LORD Flocklok® 7000/7204 adhesive is a two-part, single-coat adhesive used for adhering polyester or nylon flock fibers to a variety of thermoplastics, including PVC, Alcryn®, Sunprene®, ny.. |
|||
Flash Point | 27.0 °C | 80.6 °F | closed cup |
Dow Corning 805 RESIN Silicone binder resin for maintenance paints, colored baking enamels, decorative finishes; primarily with metallic pigments. Used alone or blended with Dow Corning® 806A Resin to promote intermedia.. |
|||
Flash Point | 27.0 °C | 80.6 °F | closed cup |
Dow Corning 808 RESIN Medium-soft, silicone resin binder for heat resistant maintenance paints and colored baking enamels.Information provided by Dow Corning |
|||
Flash Point | 27.0 °C | 80.6 °F | closed cup |
Dow Corning HV 1860/120 PRIMER Primer designed for use with peroxide curing silicone rubbers to provide good bonding to metal, glass fibre and epoxy resinInformation provided by Dow Corning |
|||
Flash Point | 27.0 °C | 80.6 °F | closed cup |
Dow Corning Q2-7406 ADHESIVE Dow Corning® Q2-7406 Adhesive is a polydimethylsiloxane gum and resin dispersion; provides excellent high temperature properties with adhesion to 288C (550F).Information provided by Dow Corning |
|||
Flash Point | 27.0 °C | 80.6 °F | closed cup |
Dow Corning Q2-7566 ADHESIVE Dow Corning® Q2-7566 Adhesive is a high viscosity, polydimethylsiloxane gum and resin dispersion, providing excellent high temperature properties with adhesion to 288C (550F).Information provided b.. |
|||
Flash Point | 27.0 °C | 80.6 °F | closed cup |
Dow Corning Q2-7735 ADHESIVE Dow Corning® Q2-7735 Adhesive is a polydimethylsiloxane gum and resin dispersion, and provides high tack combined with good adhesion.Information provided by Dow Corning |
|||
Flash Point | >= 27.0 °C | >= 80.6 °F | closed cup |
Dow Corning SYL-OFF® 23A CATALYST Liquid. Standard cure. A 50% solids dispersion of an organotin complex in xylene.Information provided by Dow Corning |
|||
Flash Point | 27.0 °C | 80.6 °F | closed cup |
Dow Corning SYL-OFF® C4-2109 RELEASE ADDITIVE C4-2109 is a 10% active solids solution of a silicate based compound. This product is recommended for use as a release modifier for Syl-Off® brand solvent based, condensation curing, systems.Inform.. |
|||
Flash Point | 27.0 °C | 80.6 °F | closed cup |
Dow Corning Z-6264 SILANE Dow Corning® Z-6264 Silane is an alkylalkoxysilane. It has an n-propyl organic group and a trimethoxysilyl inorganic group.Information provided by Dow Corning |
|||
Flash Point | 27.0 °C | 80.6 °F | closed cup |
Dow Corning 1-6184 WATER REPELLENT Dow Corning® 1-6184 Water Repellent is a low-VOC, multifunctional, self-crosslinking, water soluble siloxaneInformation provided by Dow Corning |
|||
Flash Point | 27.0 °C | 80.6 °F | |
Dow Corning 1250 SURFACTANT 50% silicone resin in Xylene solvent. Silicone Profoamer for mechanically frothing PVC dispersions. Good foam control for PVC foam coatings. Better water resistance and less odor than alkali metal s.. |
|||
Flash Point | 27.0 °C | 80.6 °F | closed cup |
Dow Corning 409 HS RESIN High-performance coatings; high-temperature applications where low VOC content is required. Used alone or blended with a variety of solvent-based silicone and organic resins. Similar to Dow Corning®.. |
|||
Flash Point | 27.0 °C | 80.6 °F | |
BASF 3-Methoxypropylamine (MOPA) Formula: C4H11NOCAS: 5332-73-0Description: 3-Methoxypropylamine (MOPA) is a colorless to yellow liquid with an aminelike odor. It is miscible in water.Synonyms: 3-Aminopropyl methyl ether, 3-Methox.. |
|||
Flash Point | 27.0 °C | 80.6 °F | |
BASF Cyclopentanone Formula: C5H8OCAS: 120-92-3Description: Cyclopentanone is a water-white liquid, soluble in water, alcohol and ether.Applications: Intermediate used in the production of pharmaceuticals, biologicals,.. |
|||
Flash Point | 27.0 °C | 80.6 °F | |
BASF Cyclohexylamine (CHA) Formula: C6H13NCAS: 108-91-8Description: Cyclohexylamine i(CHA) s a colorless to yellow liquid with an amine-like odor. It is miscible with water.Synonyms: CHA, Cyclohexylamine, Cyclohexyl amine, 1-.. |