Material Notes:
Formula: C4H11NOCAS: 5332-73-0Description: 3-Methoxypropylamine (MOPA) is a colorless to yellow liquid with an aminelike odor. It is miscible in water.Synonyms: 3-Aminopropyl methyl ether, 3-Methoxy-1-propanamine, 1-Amino-3-methoxypropane, 3-Methoxy-n-propylaminlApplications: Intermediate used in the production of: Corrosion inhibitor and DyestuffInformation provided by BASF
Physical Properties Metric English Comments
Density 0.872 g/cc
0.0315 lb/in³
Molecular Weight 89.1 g/mol
89.1 g/mol
Thermal Properties Metric English Comments
Melting Point <= -70.0 °C
<= -94.0 °F
Freezing Point
Boiling Point 118 °C
244 °F
Flash Point 27.0 °C
80.6 °F
Processing Properties Metric English Comments
Moisture Content <= 0.50 %
<= 0.50 %
DIN 51 777
Descriptive Properties Value Comments
Assay >99%
Color <15
APHA, DIN EN 1557
Ignition Temperature 270°C
Copyright © lookpolymers.com All Rights Reserved