Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Palm Labs Adhesives TURBO-LOCK SERIES 15 Anaerobic Thread Locking Compound

Category Polymer , Adhesive , Thermoset , Methacrylate , Methacrylate Adhesive
Manufacturer Palm Labs Adhesives
Trade Name TURBO-LOCK SERIES
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Palm Labs Adhesives TURBO-LOCK SERIES 15 Anaerobic Thread Locking Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TURBO-LOCK 15 SERIES is a fast curing, large bolt, RED, high strength, anaerobic thread-locking compound for bonding and sealing threads. Prevents rusting of threads. It is highly resistance to heat, vibrations, water, gases, oils, hydrocarbons and many chemicals. Disassembles with heat and hand tools.Applications:Ideal for locking and sealing of larger bolts and studs (25 mm and larger).Transmission and engine block studs, valve sets, etc.High strength, large bolt, permanent and eliminates need for double nutting and welding. Prevents corrosion and leakage.Excellent performance of even oily surfaces.Fasteners on vibrating machines or moving components.Meets Military Specification: MIL-S-43163Part Numbers for this data: 14-000, 14-001, 14-010, 14-050, 14-250, 14-1000Information provided by Palm Laboratories Adhesives
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
Brookfield Viscosity 7000 cP
7000 cP
RVT Spindle 3 @ 20 rpm
Mechanical Properties Metric English Comments
Shear Strength >= 9.00 MPa
>= 1310 psi
ISO 10123; Compressive, Steel pins and collars
Thermal Properties Metric English Comments
CTE, linear 0.800 µm/m-°C
0.444 µin/in-°F
ASTM D696
Specific Heat Capacity 0.300 J/g-°C
0.0717 BTU/lb-°F
Thermal Conductivity 0.100 W/m-K
0.694 BTU-in/hr-ft²-°F
ASTM C177
Flash Point >= 37.8 °C
>= 100 °F
Processing Properties Metric English Comments
Cure Time 120 - 240 min
2.00 - 4.00 hour
Functional
1440 min
24.0 hour
Full
30.0 min

@Temperature -55.0 - 150 °C
0.500 hour

@Temperature -67.0 - 302 °F
Handling
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Red
Chemical Resistance 100% Initial Strength Retained
Motor Oil at 125°C, at 500hrs
100% Initial Strength Retained
Gasoline at 22°C, at 500hrs
100% Initial Strength Retained
Motor Oil at 125°C, at 1000hrs
100% Initial Strength Retained
Gasoline at 22°C, at 1000hrs
90% Initial Strength Retained
Brake Fluid at 22°C, at 1000hrs
90% Initial Strength Retained
Water/Glycol at 87°C, at 1000hrs
90% Initial Strength Retained
Brake Fluid at 22°C, at 500hrs
90% Initial Strength Retained
Water/Glycol at 87°C, at 500hrs
95% Initial Strength Retained
Acetone at 22°C, at 1000hrs
95% Initial Strength Retained
Ethanol at 22°C, at 1000hrs
95% Initial Strength Retained
Acetone at 22°C, at 500hrs
95% Initial Strength Retained
Ethanol at 22°C, at 500hrs
Composition Methacrylate Ester
Max Screw Size 1 ½” / 36 mm
Torque 32 N.m
Breakaway, M10 steel nuts and bolts N.m, ISO 10964
32 N.m
Prevail, M10 steel nuts and bolts N.m, ISO 10964
38 N.m
Breakloose, pre-torqued to 5 N.m, M10 steel nuts and bolts, ISO 10964
40 N.m
Max Prevail, pre-torqued to 5 N.m, M10 steel nuts and bolts N.m, ISO 10964
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved