Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 55.0 - 85.0 °C | 131 - 185 °F | |
M Chemical GUARD DOGâ„¢ UV622 HALS Light Stabilizer GUARD DOGâ„¢ UV662 is a solid, polymeric type, free radical scavenger hindered amine light stabilizer that is used to protect a wide range of polymers against degradation caused by exposure to UV.. |
|||
Softening Point | 80.0 - 85.0 °C | 176 - 185 °F | MQSA 70A |
Lubrizol Advanced Materials Pearlbond® D1160 Thermoplastic Polyurethane Pearlbond™ D1160 is a linear, aromatic polyurethane, supplied in form of small white granules, which combines a high crystallization rate and high thermoplasticity level. Applications: Pearlbo.. |
|||
Softening Point | 60.0 - 85.0 °C | 140 - 185 °F | |
Aquabond Technologies Aquabond™ ABS-85 Water Soluble Adhesive and Bonding Thermoplastic Description: Aquabond's water soluble thermoplastic is designed for temporary mounting of hard materials for slicing, dicing, grinding, lapping and polishing and comes in 3 different bonding tem.. |