Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 60.0 - 70.0 °C | 140 - 158 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 115 Linear Thermoplastic Polyurethane
(discontinued **) PEARLBOND® 115 is a linear, aromatic polyurethane, supplied in form of white slightly yellowish pellets, which combines a very high crystallization rate with a high thermoplasticity level.Applicati.. |
|||
Softening Point | 60.0 °C | 140 °F | Flow beginning temperature |
Wanhua Chemical Wanthane® WHT-6290 TPU Hot-Melt Adhesive Wide range of activation temperature, fast crystallization rate, outstanding bonding strength for fabrics, leathers, plastics & rubbers, wood, etc.Information provided by Wanhua Chemical Group Co., .. |
|||
Softening Point | 60.0 - 85.0 °C | 140 - 185 °F | |
Aquabond Technologies Aquabond™ ABS-85 Water Soluble Adhesive and Bonding Thermoplastic Description: Aquabond's water soluble thermoplastic is designed for temporary mounting of hard materials for slicing, dicing, grinding, lapping and polishing and comes in 3 different bonding tem.. |
|||
Softening Point | 60.0 - 70.0 °C | 140 - 158 °F | |
Beijing Ranger Chem E-21 Solid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Softening Point | 60.0 - 76.0 °C | 140 - 169 °F | |
Beijing Ranger Chem SM-601 Solid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Softening Point | 60.0 - 70.0 °C | 140 - 158 °F | Kofler; MQSA 70 A |
Lubrizol Advanced Materials Pearlbond® D183 Thermoplastic Polyurethane
(discontinued **) The Pearlbond® grades are aromatic crystalline TPUs used for the production of heat activated shoe counters and toe puffs, and orthopedic products. The Pearlbond® grades are supplied in pellet fo.. |