Thermal Properties Metric English Comments
Softening Point 80.0 °C
176 °F
ISO 306
Iran Petrochemical (PCC) BL 4M HM 8355 High Density Polyethylene
BL4M is a high density polyethylene with 1-Butene as co monomer. It is high molar mass, easily processable, high stiffness and strength, good SCR, very good molding surface finish.Applications: jer..
Softening Point 80.0 °C
176 °F
ISO 306
Iran Petrochemical (PCC) EX 2 HF 7750 M High Density Polyethylene
EX2 is a high density polyethylene with 1-Butene as co monomer. It has good rigidity and medium molar mass. Applications: monofilaments, ropes, yarns.Information provided by Iran Petrochemical Com..
Softening Point 80.0 °C
176 °F
ISO 306
Iran Petrochemical (PCC) EX 2 S HF 7750 M2 High Density Polyethylene
EX2S is a high density polyethylene with 1-Butene as co monomer. It is medium molar mass, low density grade with a narrow molar mass distribution, high rigidity, good tear strength. Applications: ..
Softening Point 80.0 - 85.0 °C
176 - 185 °F
MQSA 70A
Lubrizol Advanced Materials Pearlbond® D1160 Thermoplastic Polyurethane
Pearlbondâ„¢ D1160 is a linear, aromatic polyurethane, supplied in form of small white granules, which combines a high crystallization rate and high thermoplasticity level. Applications: Pearlbo..
Softening Point 80.0 - 100 °C
176 - 212 °F
Lucobit Lucobit® 1210A Ethylene Copolymer Bitumen
Lucobit 1210A is a mixture of ethylene copolymers and special bitumen. Addition of Lucobit to bitumen increases its viscosity and broadens the range of plasticity.Lucobit 1210A in asphalt mixtures ..
Softening Point 80.0 - 100 °C
176 - 212 °F
Lucobit Lucolast® 7010 Ethylene Butyl Acrylate Asphalt Additive
Lucolast® 7010 is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Addition of Lucolast 7010 to bitumen increases its viscosity, broadens the range of plasticit..
Softening Point 80.0 °C
176 °F
ISO 306
Iran Petrochemical (PCC) BL 3VD HH 4765 High Density Polyethylene
BL3VD is a high density polyethylene with 1-Butene as co monomer. It is very high density and stiffness, good ESCR, high flowability and impact strength.Applications: small blow molding, bottles, c..
Softening Point 80.0 - 100 °C
176 - 212 °F
flow beginning
Taiwan Sheen Soon Sheenthane® AH-580 TPU for Hotmelt Adhesive
Thermoplastic polyurethane elastomer for soft hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes..
Softening Point 80.0 °C
176 °F
Struktol VP 3735 Flame retarded epoxy resin
Applications: STRUKTOL VP 3735 is a multifunctional epoxy resin, which contains a chemically bound organophosphorous substance. Thus the mechanical properties like tenacity and modulus are not influ..
Softening Point 80.0 - 100 °C
176 - 212 °F
flow beginning
Taiwan Sheen Soon Sheenthane® AH-500 TPU for Hotmelt Adhesive
Thermoplastic polyurethane elastomer for soft hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes..
Softening Point 80.0 - 100 °C
176 - 212 °F
flow beginning
Taiwan Sheen Soon Sheenthane® AH-562 TPU for Hotmelt Adhesive
Thermoplastic polyurethane elastomer for soft hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes..
Softening Point 80.0 °C
176 °F
JIS K-2531
Unitika elitel UE3300 Polyester, Flake
Low molecular weight type UE3210, High OH type, Branched & highly crosslinkedUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications fro..
Softening Point 80.0 °C
176 °F
Zeon Chemicals Quintone® N180 Aliphatic Hydrocarbon Resin
C5/C9 type (piperylene and dicyclopentadiene precursor). Gives excellent tackiness to adhesives, especially suitable for hot-melt adhesives.Information provided by Zeon Chemicals L.P.
Softening Point 80.0 - 100 °C
176 - 212 °F
flow beginning
Taiwan Sheen Soon Sheenthane® AH-560T TPU for Hotmelt Adhesive
Thermoplastic polyurethane elastomer for soft hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes..