Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 55.0 - 85.0 °C | 131 - 185 °F | |
M Chemical GUARD DOGâ„¢ UV622 HALS Light Stabilizer GUARD DOGâ„¢ UV662 is a solid, polymeric type, free radical scavenger hindered amine light stabilizer that is used to protect a wide range of polymers against degradation caused by exposure to UV.. |
|||
Softening Point | 55.0 - 60.0 °C | 131 - 140 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 100 Linear Thermoplastic Polyurethane Pearlbond™ 100 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines a very high crystallization rate with a very high thermoplasticity leve.. |
|||
Softening Point | 55.0 - 60.0 °C | 131 - 140 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 106 Linear Thermoplastic Polyurethane Pearlbond™ 106.is a linear, aromatic polyurethane, supplied in form of small white or slightly yellowish granules, which combines a high crystallisation rate with a very high thermoplasticity l.. |
|||
Softening Point | 55.0 - 60.0 °C | 131 - 140 °F | Kolfer; MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 120 Linear Thermoplastic Polyurethane Pearlbond® 120 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines an extremely high crystallization rate with a very high thermoplasticity .. |
|||
Softening Point | 55.0 - 60.0 °C | 131 - 140 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 121 Linear Thermoplastic Polyurethane Pearlbond™ 121 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines an extremely high crystallization rate with a very high thermoplasticit.. |
|||
Softening Point | 55.0 - 60.0 °C | 131 - 140 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 122 Linear Thermoplastic Polyurethane Pearlbond™ 122 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines an extremely high crystallization rate with a very high thermoplasticit.. |
|||
Softening Point | 55.0 - 60.0 °C | 131 - 140 °F | MQSA 70 A |
Lubrizol Advanced Materials Pearlbond® 180 Thermoplastic Polyurethane Pearlbond™ 180 is a linear, polyester-based polyurethane, supplied in form of small white granules, which combines a very high crystallization rate with a very high thermoplasticity level. It i.. |
|||
Softening Point | 55.0 - 60.0 °C | 131 - 140 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 101 Linear Thermoplastic Polyurethane Pearlbond™ 101 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines a very high crystallization rate with a very high thermoplasticity leve.. |
|||
Softening Point | 55.0 - 60.0 °C | 131 - 140 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 123 Linear Thermoplastic Polyurethane Pearlbond™ 123 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines an extremely high crystallization rate with a very high thermoplasticit.. |
|||
Softening Point | 55.0 - 60.0 °C | 131 - 140 °F | |
Aquabond Technologies Aquabond™ ABS-65 Water Soluble Adhesive and Bonding Thermoplastic Description: Aquabond's water soluble thermoplastic is designed for temporary mounting of hard materials for slicing, dicing, grinding, lapping and polishing and comes in 3 different bonding tem.. |
|||
Softening Point | 55.0 - 60.0 °C | 131 - 140 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 103 Linear Thermoplastic Polyurethane Pearlbond™ 103 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines a very high crystallization rate with a very high thermoplasticity level. I.. |