Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 63.9 °C | 147 °F | ASTM D648 |
RheTech Products CC30P100-01 30% Calcium Carbonate Reinforced Polypropylene, Black Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.9 °C | 147 °F | ASTM D648 |
RheTech Products M15P101-01A 15% Mica Reinforced Polypropylene, Black Applications: Air ducts - distributionFan shroudsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.9 °C | 147 °F | ASTM D648 |
RheTech Products M15P101-01 15% Mica Reinforced Polypropylene, Black Applications: Air ducts - distributionFan shroudsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.9 °C | 147 °F | Unannealed; ISO 75-2/A |
Ravago Manufacturing Americas Hylon® N1000STHL HF Nylon 6/6
(discontinued **) Available in North America Additive: Heat Stabilizer and LubricantFeatures: Lubricated, Heat Stabilized, High Flow and Ultra High ToughnessRoHS CompliantAuto Specifications: DELPHI DCM 4849 Color: B.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.9 °C | 147 °F | Unannealed; ISO 75A-1, -2 |
LyondellBasell Hostacomâ„¢ TRC704D Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ TRC704D medium high melt flow, 1,500 MPa flexural modulus, UV-stabilized thermoplastic elastomeric olefin (TEO) resin has an excellent combination of properties and proce.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.9 °C | 147 °F | ISO 75-2/A |
ExxonMobil Exxtral™ HMU 208 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin, black colored, with high stiffness and release agent for automotive HVAC and under-the-hood applications.Availability: Africa & Middl.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.9 °C | 147 °F | ISO 75-2/A |
ExxonMobil Exxtral™ HMU 210 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin, black colored, with high stiffness for automotive HVAC and under-the-hood applications.Availability: Africa & Middle East, Asia Pacif.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.9 °C | 147 °F | ISO 75-2/A |
ExxonMobil Exxtral™ HMU 234 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin, black colored, with high stiffness, high heat stabilization, low emissions and low odor for automotive HVAC and under-the-hood applic.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.9 °C | 147 °F | ISO 75-2/A |
ExxonMobil Exxtral™ HMU 301 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for high heat and discoloration resistance, good surface finish, and detergent resistance for electrical appliances such as w.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.9 °C | 147 °F | |
Aclo Accutech Polypropylene Homopolymer HP0334W20L1 Wollastonite Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.9 °C | 147 °F | ASTM D648 |
Asahi Kasei Thermylene® P6-30FG-0602 30% Glass Fiber Reinforced, UV Stabilized Information provided by Asahi Thermofil |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.9 °C | 147 °F | ASTM D-648 |
Axiall 8258 Rigid PVC, Extrusion Georgia Gulf 8258 is a special purpose rigid PVC for film and food grade sheet compound. It has been used where packages are manufactured to FDA guidelines.Information provided by Georgia GulfGeorg.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.9 °C | 147 °F | ASTM D648 |
Asahi Kasei Thermylene® P7-20FG-0610 20% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.9 °C | 147 °F | ASTM D648 |
RheTech Products CC30P100-00 30% Calcium Carbonate Reinforced Polypropylene, Natural Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |