Material Notes:
Product Description: A specialty thermoplastic polyolefin resin, black colored, with high stiffness and release agent for automotive HVAC and under-the-hood applications.Availability: Africa & Middle East, Asia Pacific, Europe, South America and North America Features: Good Dimensional StabilityGood Mold ReleaseUltra High StiffnessUses: Automotive ApplicationsAutomotive Exterior PartsAutomotive Exterior TrimAutomotive Interior PartsAutomotive Under the Hood Compounding Processing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ISO 1183
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 27.0 MPa
3920 psi
ISO 527-2/50
Tensile Strength, Yield 34.0 MPa
4930 psi
ISO 527-2/50
Elongation at Break 19 %
19 %
ISO 527-2/50
Elongation at Yield 4.0 %
4.0 %
ISO 527-2/50
Tensile Modulus 2.75 GPa
399 ksi
Secant; ISO 527-2
Charpy Impact Unnotched 3.57 J/cm²
17.0 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.294 J/cm²

@Temperature 22.8 °C
1.40 ft-lb/in²

@Temperature 73.0 °F
Complete Break; ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 120 °C
248 °F
ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 63.9 °C
147 °F
ISO 75-2/A