Material Notes:
Product Description: A specialty thermoplastic polyolefin resin designed for high heat and discoloration resistance, good surface finish, and detergent resistance for electrical appliances such as washing machines. Contains an anti-static additive.Availability: Africa & Middle East, Asia Pacific, Europe, South America and North America Features: Good ColorabilityGood Dimensional StabilityGood Surface FinishHigh FlowUltra High StiffnessUses: Appliance ComponentsAppliancesConsume Applications Processing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183
Melt Flow 14 g/10 min

@Load 2.16 kg,
Temperature 230 °C
14 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 30.0 MPa
4350 psi
ISO 527-2/50
Tensile Strength, Yield 33.4 MPa
4840 psi
ISO 527-2/50
Elongation at Break 9.0 %
9.0 %
ISO 527-2/50
Elongation at Yield 3.0 %
3.0 %
ISO 527-2/50
Tensile Modulus 3.30 GPa
479 ksi
Secant; ISO 527-2
Flexural Modulus 3.30 GPa
479 ksi
ISO 178
Charpy Impact, Notched 0.357 J/cm²

@Temperature 22.8 °C
1.70 ft-lb/in²

@Temperature 73.0 °F
Complete Break; ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 120 °C
248 °F
ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 63.9 °C
147 °F
ISO 75-2/A