Material Notes:
Georgia Gulf 8258 is a special purpose rigid PVC for film and food grade sheet compound. It has been used where packages are manufactured to FDA guidelines.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 46.2 MPa
6700 psi
ASTM D-638
Tensile Modulus 2.48 GPa
360 ksi
ASTM D-638
Flexural Strength 82.7 MPa
12000 psi
ASTM D-790
Izod Impact, Notched 1.33 J/cm

@Thickness 3.17 mm
2.50 ft-lb/in

@Thickness 0.125 in
ASTM D-256
Tensile Impact Strength 158 kJ/m²
75.0 ft-lb/in²
ASTM D-1822
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 63.9 °C
147 °F
ASTM D-648
Optical Properties Metric English Comments
Haze 5.0 %
5.0 %
ASTM D-1003-61
Transmission, Visible 77 %
77 %
ASTM D-1003-61
Descriptive Properties Value Comments
Equilibrium Torque, meter-grams 1400
Brabender Plastograph, No. 6, Roller Head, 190°C, 57-g, Charge, 100rpm
Stability Time, minutes 21