Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 272 °C
522 °F
Unannealed; ASTM D648
PolyOne Edgetek® SF2-40CF/000 NATURAL Polyphenylene Sulfide (PPS)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Deflection Temperature at 1.8 MPa (264 psi) 272 °C

@Thickness 3.20 mm
522 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP KONDUIT OTF2AXXP PPS (Asia Pacific)
LNP* Konduit* OTF2AXXP is a compound based on Polyphenylene Sulfide resin containing Glass Fiber, Thermal Carbon Fiber. Added features of this material include: Thermally Conductive, Electrically C..
Deflection Temperature at 1.8 MPa (264 psi) 272 °C
522 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP THERMOCOMP OF008A PPS (Asia Pacific)
LNP* Thermocomp* OF008A is a compound based on PPS - Branched resin containing Glass Fiber.This product is also known as Thermocomp* OF-1008.
Deflection Temperature at 1.8 MPa (264 psi) 272 °C
522 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP THERMOCOMP OF008AH PPS - Branched
LNP* THERMOCOMP* OF008AH is a compound based on PPS - Branched resin containing 40% Glass Fiber. Added features of this grade are: Healthcare.
Deflection Temperature at 1.8 MPa (264 psi) 272 °C
522 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP Thermocomp OF008E PPS
LNP* Thermocomp* OF008E is a compound based on Polyphenylene Sulfide resin containing Glass Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the A..
Deflection Temperature at 1.8 MPa (264 psi) 272 °C
522 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP THERMOCOMP OF008E PPS - LINEAR
LNP* THERMOCOMP* OF008E is a compound based on PPS - Linear resin containing 40% Glass Fiber. Added features of this material include: Easy Molding.
Deflection Temperature at 1.8 MPa (264 psi) 272 °C
522 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP THERMOCOMP OF008E PPS (Asia Pacific)
LNP* Thermocomp* OF008E is a compound based on Polyphenylene Sulfide resin containing Glass Fiber. Added features of this material include: Easy Molding.
Deflection Temperature at 1.8 MPa (264 psi) 272 °C
522 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP THERMOCOMP UF008H PPA
LNP THERMOCOMP* UF008H is a compound based on Polyphthalamide resin containing 40% Glass Fiber. Added feature of this grade is: Healthcare.
Deflection Temperature at 1.8 MPa (264 psi) 272 °C
522 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP THERMOCOMP UF00BAS PPA
LNP* THERMOCOMP* UF00BAS is a compound based on Polyphthalamide containing 55% Glass Fiber. Added feature of this material is: Heat Stabilized.
Deflection Temperature at 1.8 MPa (264 psi) 272 °C
522 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP THERMOCOMP OF008A PPS - Branched
LNP* THERMOCOMP* OF008A is a compound based on PPS - Branched resin containing 40% Glass Fiber.
Deflection Temperature at 1.8 MPa (264 psi) 272 °C
522 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP THERMOCOMP OF008A PPS - Branched (Europe-Africa-Middle East)
LNP* Thermocomp* OF008A is a compound based on PPS - Branched resin containing Glass Fiber.
Deflection Temperature at 1.8 MPa (264 psi) 272 °C
522 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP THERMOCOMP UF008H PPA (Asia Pacific)
LNP THERMOCOMP* UF008H is a compound based on Polyphthalamide resin containing Glass Fiber.
Deflection Temperature at 1.8 MPa (264 psi) 272 °C
522 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP VERTON UV00AS PPA (Asia Pacific)
LNP* Verton* UV00AS is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized.
Deflection Temperature at 1.8 MPa (264 psi) 272 °C
522 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP VERTON UV00ASU PPA
LNP* VERTON* UV00ASU is a compound based on Polyphthalamide resin containing 50% Long Glass Fiber. Added features of this material include: UV Stabilized, Heat Stabilized, Structural.
Deflection Temperature at 1.8 MPa (264 psi) 272 °C
522 °F
ASTM D648
Plenco 08133 Polyester BMC, Compression Molded
PLENCO 08133 is a renumber of PlasGlas 10313. PLENCO 08133 is a general purpose polyester bulk molding compound that is characterized by adding utility to a number of applications. Because of its co..
Deflection Temperature at 1.8 MPa (264 psi) 272 °C
522 °F
Unannealed; ASTM D648
LNP Konduit® OTF-202-10 Polyphenylene Sulfide, Carbon Fiber Reinforcement  (discontinued **)
Features: Electrically Conductive, Thermally ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; h..
Deflection Temperature at 1.8 MPa (264 psi) 272 °C
522 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP VERTON UV00AS PPA
LNP* VERTON* UV00AS is a compound based on Polyphthalamide resin containing 50% Long Glass Fiber. Added features of this material include: Heat Stabilized, Structural.