Category Polymer , Thermoset , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester Glass Filled BMC
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 08133 Polyester BMC, Compression Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 08133 is a renumber of PlasGlas 10313. PLENCO 08133 is a general purpose polyester bulk molding compound that is characterized by adding utility to a number of applications. Because of its combination of high heat resistance, good electrical properties, flame resistance and strength, it can be used in such applications as iron skirts and other small appliance housings, coil bobbins, and electric motor components such as brush holders. It is available in either bulk or extruded form and is currently available in black. Other colors are available upon request. It is UL recognized under file E40654.Information supplied by Plenco.
Physical Properties Metric English Comments
Density 1.85 g/cc
0.0668 lb/in³
ASTM D792
Water Absorption 0.065 %
0.065 %
ASTM D570
Linear Mold Shrinkage 0.0037 cm/cm
0.0037 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 40
40
ASTM D785
Tensile Strength, Ultimate 37.0 MPa
5370 psi
ASTM D638
Elongation at Break 0.52 %
0.52 %
ASTM D638
Tensile Modulus 12.7 GPa
1840 ksi
ASTM D638
Flexural Strength 99.0 MPa
14400 psi
ASTM D790
Flexural Modulus 11.6 GPa
1680 ksi
ASTM D790
Compressive Strength 134 MPa
19400 psi
ASTM D695
Izod Impact, Notched 2.22 J/cm
4.16 ft-lb/in
ASTM D256
Charpy Impact, Notched 2.35 J/cm²
11.2 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 218 °C
424 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 272 °C
522 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
Shrinkage 0.00 %
0.00 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 2.40e+11 ohm-cm
2.40e+11 ohm-cm
ASTM D247
Dielectric Constant 19.1
19.1
ASTM D150
Dielectric Strength 2.61 kV/mm
66.3 kV/in
Short Time; ASTM D149
5.80 kV/mm
147 kV/in
Step by Step; ASTM D149
Dissipation Factor 0.40
0.40
ASTM D150
Arc Resistance 180 sec
180 sec
ASTM D495
Comparative Tracking Index 600 V
600 V
ASTM D3638