Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 50.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 45.0 - 50.0 °C
113 - 122 °F
ASTM D648-07
Proto3000 Objet FullCure720 Transparent Prototyping Polymer
Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid ..
Deflection Temperature at 1.8 MPa (264 psi) 45.0 - 50.0 °C
113 - 122 °F
ASTM D648-07
Proto3000 Objet VeroBlack FullCure870 Rigid Opaque Prototyping Polymer
Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid ..
Deflection Temperature at 1.8 MPa (264 psi) 45.0 - 50.0 °C
113 - 122 °F
ASTM D648-07
Proto3000 Objet VeroBlue FullCure840 Rigid Opaque Prototyping Polymer
Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid ..
Deflection Temperature at 1.8 MPa (264 psi) 45.0 - 50.0 °C
113 - 122 °F
ASTM D648-07
Proto3000 Objet VeroClear FullCure810
Information provided by Proto3000 for their protoyping engineering services.
Deflection Temperature at 1.8 MPa (264 psi) 45.0 - 50.0 °C
113 - 122 °F
ASTM D648-07
Proto3000 Objet VeroGray FullCure850 Rigid Opaque Prototyping Polymer
Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid ..
Deflection Temperature at 1.8 MPa (264 psi) 48.0 - 50.0 °C
118 - 122 °F
ASTM D648-98c
DSM Somos® ProtoGen™ O-XT 18120 Epoxy Resin for Stereolithography, UV Postcure at HOC -2
DescriptionDSM Somos® ProtoGen O-XT 18120 is a liquid photopolymer that produces accurate parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demonstrate diffe..
Deflection Temperature at 1.8 MPa (264 psi) 49.0 - 50.0 °C
120 - 122 °F
Thermal Postcure; ASTM D648-98c
DSM Somos® WaterClear® Ultra 10122 Optically Clear, Colorless, Rigid, Stereolithography Resin
DescriptionDSM Somos® WaterClear Ultra 10122 is a next generation optically clear resin with ABS like properties and good temperature resistance. It produces colorless, functional, accurate parts ..
Deflection Temperature at 1.8 MPa (264 psi) 48.0 - 50.0 °C
118 - 122 °F
ASTM D648
3D Systems Accura® 60 Plastic for SLA® Systems
Simulate the properties and appearance of polycarbonate. For use with solid-state stereolithography (SLA®) systems.ApplicationsTough functional prototypesAutomotive design componentsConsumer electr..
Deflection Temperature at 1.8 MPa (264 psi) 48.0 - 50.0 °C
118 - 122 °F
ASTM D648
Proto3000 Accura® 60 Plastic Stereolithography (SLA) Prototyping Polymer
Features:Durable and stiffHigh clarityFast build speedLow viscosity formulationHumidity resistant partsFully developed and tested build stylesBenefits:Achieve the look and feel of polycarbonateView ..
Deflection Temperature at 1.8 MPa (264 psi) 45.0 - 50.0 °C
113 - 122 °F
ASTM D648-07
Proto3000 Objet VeroWhitePlus FullCure835 Rigid Opaque Prototyping Polymer
Information provided by Proto3000 for their protoyping engineering services.