3D Systems Accura® 60 Plastic for SLA® Systems

Category Polymer , Rapid Prototyping Polymer
Manufacturer 3D Systems Corporation
Trade Name Accura®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3D Systems Accura® 60 Plastic for SLA® Systems.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Simulate the properties and appearance of polycarbonate. For use with solid-state stereolithography (SLA®) systems.ApplicationsTough functional prototypesAutomotive design componentsConsumer electronics (cell phones etc.)Medical instruments, devices and labwareLighting components (lenses etc.)Fluid flow and visualization modelsMaster patterns for urethane castingsQuickCast™ patterns for investment castingTransparent assembliesClear display modelsConcept and marketing modelsAll information provided by 3D Systems.
Physical Properties Metric English Comments
Density 1.13 g/cc

@Temperature 25.0 °C
0.0408 lb/in³

@Temperature 77.0 °F
Liquid
1.21 g/cc

@Temperature 25.0 °C
0.0437 lb/in³

@Temperature 77.0 °F
Solid
Viscosity 150 - 180 cP

@Temperature 30.0 °C
150 - 180 cP

@Temperature 86.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 86
86
Tensile Strength, Yield 58.0 - 68.0 MPa
8410 - 9860 psi
ASTM D638
Elongation at Break 5.0 - 13 %
5.0 - 13 %
ASTM D638
Tensile Modulus 2.69 - 3.10 GPa
390 - 450 ksi
ASTM D638
Flexural Strength 87.0 - 101 MPa
12600 - 14600 psi
ASTM D790
Flexural Modulus 2.70 - 3.00 GPa
392 - 435 ksi
ASTM D790
Izod Impact, Notched 0.150 - 0.250 J/cm
0.281 - 0.468 ft-lb/in
ASTM D256
Penetration 6.3
6.3
mils
Thermal Properties Metric English Comments
CTE, linear 71.0 µm/m-°C

@Temperature 0.000 - 40.0 °C
39.4 µin/in-°F

@Temperature 32.0 - 104 °F
T<Tg; ASTM E831-93
153 µm/m-°C

@Temperature 75.0 - 140 °C
85.0 µin/in-°F

@Temperature 167 - 284 °F
T>Tg; ASTM E831-93
Deflection Temperature at 0.46 MPa (66 psi) 53.0 - 55.0 °C
127 - 131 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 48.0 - 50.0 °C
118 - 122 °F
ASTM D648
Glass Transition Temp, Tg 58.0 °C
136 °F
DMA, E"
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Descriptive Properties Value Comments
Appearance Clear
Critical Exposure (mJ/cm²) 7.6
Tested Build Styles FAST™, EXACT™, and QuickCast™