Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 335 °C | 635 °F | ISO 75-f |
Victrex® PEEK 150GL30 30% Glass Fiber Reinforced Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact c.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 335 °C | 635 °F | ISO 75A-f |
Victrex® PEEK 90GL30 BLACK EU 30% Glass Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, FDA and EU food contact compliant, .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 335 °C | 635 °F | ISO 75A-f |
Victrex® PEEK 90GL30 Polyetheretherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 335 °C | 635 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP LUBRICOMP LX91475 PEEK LNP* LUBRICOMP* LX91475 is a compound based on Polyetheretherketone resin containing proprietary fillers. Added features of this material include: Easy Molding, High Temperature Bearing Grade, Wear.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 335 °C @Thickness 3.20 mm |
635 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP LC008EXQ PEEK LNP* THERMOCOMP* LC008EXQ is a compound based on Polyetheretherketone containing 40% Carbon Fiber. Added features of this grade include: Electrically Conductive, Easy Molding. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 335 °C @Thickness 3.20 mm |
635 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP LC00APXQ PEEK LNP* THERMOCOMP* LC00APXQ is a compound based on Polyetheretherketone resin containing 50% Carbon Fiber. Added features of this material include: Exceptional Processing, Electrically Conductive. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 335 °C | 635 °F | ISO 75-f |
Victrex® PEEK 150GL30 Black Polyetheretherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact co.. |