Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 295 °C
563 °F
Unannealed; ISO 75-2/A
Solvay Specialty Polymers Amodel® AE-8133 Polyphthalamide (PPA)  (discontinued **)
Amodel AE-8133 is a 33% glass reinforced polyphthalamide (PPA) designed to work in the modern automotive electrical environment. This grade features a high heat deflection temperature, high flexural..
Deflection Temperature at 1.8 MPa (264 psi) 295 °C
563 °F
ASTM D648
Mitsui Arlenâ„¢ C215 15% Glass Fiber-Reinforced Modified Nylon 6T (COND)
ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss..
Deflection Temperature at 1.8 MPa (264 psi) 295 °C
563 °F
LATI Larpeek 10 G/40 PEEK, 40% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Deflection Temperature at 1.8 MPa (264 psi) 295 °C
563 °F
Unannealed; ISO 75-2/A
Solvay Specialty Polymers Amodel® A-1933 HSL Polyphthalamide (PPA), 33% Glass Fiber
Amodel® A-1933 HSL is a 33% glass reinforced grade of polyphthalamide (PPA) resin. This grade was developed specifically for improved performance in a 50/50 ethylene glycol and water environment...
Deflection Temperature at 1.8 MPa (264 psi) 295 °C

@Thickness 6.40 mm
563 °F

@Thickness 0.252 in
ASTM D648
Samsung Cheil Industries Infino® TK-4046H PPA, Glass Filled
Information provided by Samsung Cheil Industries.
Deflection Temperature at 1.8 MPa (264 psi) 295 °C

@Thickness 6.40 mm
563 °F

@Thickness 0.252 in
ASTM D648
Samsung Cheil Industries Infino® TK-4046H PPA, Glass Filled
Information provided by Samsung Cheil Industries.
Deflection Temperature at 1.8 MPa (264 psi) 295 °C
563 °F
Unannealed; Flatwise; ISO 75-2/A
Solvay Specialty Polymers Amodel® A-8950 HS Polyphthalamide (PPA), 50% Glass Fiber
Amodel® A-8950 HS is a 50% glass-fiber-reinforced, heat-stabilized polyphthalamide (PPA) with a high heat deflection temperature and very high tensile strength. Excellent creep resistance, low mo..
Deflection Temperature at 1.8 MPa (264 psi) 295 °C
563 °F
ASTM D648
DuPont Performance Polymers VESPEL TP-8161 Polyimide
DuPont Vespel TP-8161 parts are specified for high-temperature applications. TP-8161 parts offer a unique balance of mechanical and thermal properties for superior performance in aggressive environm..
Deflection Temperature at 1.8 MPa (264 psi) 295 °C
563 °F
Unannealed; ISO 75-2/A
Solvay Specialty Polymers Amodel® A-1933 HSL Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1933 HSL is a 33% glass reinforced grade of polyphthalamide (PPA) resin. This grade was developed specifically for improved performance in a 50/50 ethylene glycol and water environment. Thi..
Deflection Temperature at 1.8 MPa (264 psi) 295 °C
563 °F
LATI Latilub 88/50-20GRT K/10 PEEK, 10% Carbon Fiber Reinforced, Graphite/PTFE Filled
Self-lubricating product based on Polyetheretherketone (PEEK). Graphite / PTFE. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provid..
Deflection Temperature at 1.8 MPa (264 psi) 295 °C
563 °F
ASTM D648
Mitsui Arlen™ C215 15% Glass Fiber-Reinforced Modified Nylon 6T (DAM)
ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it possesses ..
Deflection Temperature at 1.8 MPa (264 psi) 295 °C
563 °F
ASTM D648
E-Polymers SEPAZ® C245GP 45% Glass Fiber Reinforced LCP Resin
Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding ..
Deflection Temperature at 1.8 MPa (264 psi) 295 °C
563 °F
Unannealed; ASTM D648
Solvay Specialty Polymers Amodel® AFA-4133 V0 Z Polyphthalamide (PPA), Dry  (discontinued **)
Amodel AFA-4133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar..