Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 113 - 120 °C | 235 - 248 °F | Average value: 117 °C Grade Count:3 |
Overview of materials for Polyphthalamide (PPA), High Impact This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, High Impact". Each property range of values reported is minimum and maximum values of a.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 75.0 - 120 °C | 167 - 248 °F | Average value: 88.8 °C Grade Count:92 |
Overview of materials for Polystyrene, Heat Resistant Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 104 - 120 °C | 220 - 248 °F | Average value: 112 °C Grade Count:6 |
Overview of materials for PC/ABS + Stainless Steel This property data is a summary of similar materials in the MatWeb database for the category "PC/ABS + Stainless Steel". Each property range of values reported is minimum and maximum values of appro.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 36.0 - 120 °C | 96.8 - 248 °F | Average value: 63.4 °C Grade Count:74 |
Overview of materials for Polypropylene with 10% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are .. |