Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 43.6 °C | 110 °F | ASTM D648-06 |
Objet FullCure® 830 Vero White Resin for Rapid Prototyping Information provided by American Precision Prototyping, LLC |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 43.3 °C | 110 °F | 0.125 in bar; ASTM D648 |
Network Polymers Nylon 6040 Description: Natural NylonInformation provided by Network Polymers Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 43.3 - 54.4 °C | 110 - 130 °F | ASTM D648 |
Arkema Group Kynar Flex® 3120 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 43.3 °C | 110 °F | ASTM D648 |
Global GPP-2000 Polypropylene Impact Copolymer, Cold Temperature Impact Resistant, Nucleated Information provided by Global Polymers Corporation. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 43.3 °C | 110 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® HDPE TM10 10% Talc Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 43.3 °C | 110 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® HDPE TM5 5% Talc Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 5% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 43.3 °C | 110 °F | ASTM D648 |
Spartech PE4312 Reinforced High Density Polyethylene Compound Spartech Polycom's filled high molecular weight, high density polyethylenes are specifically designed for blow molding and sheet extrusion /thermoforming of structural parts. These materials offer a.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 43.3 °C | 110 °F | ASTM D648B |
ExxonMobil HDPE HD 6733.17 High Density Polyethylene Copolymer Resin Product Description: HD 6733 is a narrow molecular weight hexane copolymer designed to maximize injection molding speed and productivity in thing wall articles. Lower processing temperatures enable .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 43.3 °C | 110 °F | ASTM D648 |
Amco PRIMATOP PP CO 200 NB Impact Polypropylene Copolymer PP CO 200 NB is cold temperature impact resistant, heat stabilized, and nucleated. Applications include toys and consumer products.Former A-Top Polymers product; part of Amco product line since 2013.. |