ExxonMobil HDPE HD 6733.17 High Density Polyethylene Copolymer Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Exxon Chemical
Trade Name HDPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil HDPE HD 6733.17 High Density Polyethylene Copolymer Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: HD 6733 is a narrow molecular weight hexane copolymer designed to maximize injection molding speed and productivity in thing wall articles. Lower processing temperatures enable production of products free of taste and odor for food and beverage packaging.Availability: Latin America, North America and South America Additive: Antioxidant: YesApplications: Food Packaging ContainersFood Service TraysHouseware ArticlesHousewares ToysInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ExxonMobil method
Melt Flow 33 g/10 min

@Load 2.16 kg,
Temperature 190 °C
33 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 0.138 MPa
20.0 psi
ASTM D638
Tensile Strength, Yield 23.4 MPa
3400 psi
ASTM D638
Flexural Modulus 0.965 GPa
140 ksi
2% Secant; ASTM D790B
Flexural Modulus, 1% Secant 1170 MPa
170000 psi
ASTM D790B
Izod Impact, Notched 0.224 J/cm

@Temperature -40.0 °C
0.420 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point <= 265 °C
<= 509 °F
Peak Melting Point; ExxonMobil method
Deflection Temperature at 0.46 MPa (66 psi) 71.7 °C
161 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 43.3 °C
110 °F
ASTM D648B