Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Global GPP-2000 Polypropylene Impact Copolymer, Cold Temperature Impact Resistant, Nucleated

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Global Polymers Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Global GPP-2000 Polypropylene Impact Copolymer, Cold Temperature Impact Resistant, Nucleated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Global Polymers Corporation.
Physical Properties Metric English Comments
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
L; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.1 MPa
3200 psi
Type 1 Specimen, Rate: 2"/min; ASTM D638
Flexural Modulus 1.07 GPa
155 ksi
ASTM D790
Izod Impact, Notched NB
NB
ASTM D256
Dart Drop, Total Energy 19.8 J

@Temperature -30.0 °C
14.6 ft-lb

@Temperature -22.0 °F
0.5 in/sec; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 79.4 °C
175 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 43.3 °C
110 °F
ASTM D648
Copyright © lookpolymers.com All Rights Reserved