Polymer Property : Brittleness Temperature = -52.6 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Brittleness Temperature -47.0 °C
-52.6 °F
ASTM D746
PolyOne Geon™ Vinyl Wire & Cable JG513GO Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Brittleness Temperature -47.0 °C
-52.6 °F
ASTM D746
S&E Specialty Polymers GTPO8102BA-H NATURAL PVC
Application: High-flow flame retardant TPO compound for insulation and jacketing compound designed for ribbon cable applications. The flame retardant package incorporates non-PDBPO, PBB, PBDE flame-..
Brittleness Temperature -47.0 °C
-52.6 °F
ASTM D746
S&E Specialty Polymers TufGuard E™ GTPO8102BA-H-Natural TPO, Flame Retardant
Application: High-flow flame retardant TPO compound for insulation and jacketing designed for ribbon cable applications. The flame retardant package incorporates non-PDBPO, PBB, PBDE flame retardant..
Brittleness Temperature -47.0 °C
-52.6 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible XV 3716 Polyvinyl Chloride, Flexible (PVC, Flexible)
A Filled PVC compound formulated specifically for FDA extrusion and Molding applications.The physical properties listed below, are typical values obtained on compression molded sheets and tested in ..
Brittleness Temperature -47.0 °C
-52.6 °F
ASTM D746
Eastman M3006-P Polyethylene  (discontinued **)
Medium density polyethylene M3006-P is a specialty formulation suggested for high speed extrusion coating applications. M3006-P offers improvements over low density polyethylene in barrier properti..
Brittleness Temperature -47.0 °C
-52.6 °F
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with Benzoflex 9-88SG Plasticizer
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Brittleness Temperature -47.0 °C
-52.6 °F
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with Cumar P-10 Plasticizer
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Brittleness Temperature -47.0 °C
-52.6 °F
ASTM D746
Teknor Apex APEX® 3201-60 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling..
Brittleness Temperature -47.0 °C
-52.6 °F
ASTM D746
Teknor Apex Flexalloy® 9604-75 Polyvinyl Chloride, Elastomer
Notes: 105°C Jacket; RoHS Compliant Features: Flame Retardant; High Heat Resistance; Low Temperature Flexibility; Sunlight Resistant (720 hours) Uses Cable Jacketing Wire Types: SEOW; SEW; SJEOW;..
Brittleness Temperature -47.0 °C
-52.6 °F
ASTM D746
Teknor Apex APEX® 1004 Polyvinyl Chloride, Flexible
Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde..
Brittleness Temperature -47.0 °C
-52.6 °F
ASTM D746
Teknor Apex APEX® 3301-60 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To..
Brittleness Temperature -47.0 °C
-52.6 °F
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with Benzoflex 9-88SG Plasticizer
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Brittleness Temperature -47.0 °C
-52.6 °F
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with Cumar P-10 Plasticizer
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Brittleness Temperature -47.0 °C
-52.6 °F
ASTM D746
ExxonMobil Santoprene® 8211-55B100 Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to ABS, PS, PC, PMMA, ASA, PET and PPO/..
Brittleness Temperature -47.0 °C
-52.6 °F
ASTM D746
Colorite Polymers MULTICHEM™ 7514 Vinyl-Urethane Blend
Description: MULTICHEM™ is characterized by:Greater ResiliencyImproved ElasticityLow Temperature PropertiesLower ExtractabilityMolding and ExtrusionInformation provided by Colorite Polymers.
Brittleness Temperature -47.0 °C
-52.6 °F
Temperature Retraction, TR-10
Dow Nordel® IP 4570 Heat Resistant Peroxide Compound
FormulationNordel® IP 4570
Brittleness Temperature -47.0 °C
-52.6 °F
ASTM D746
Colorite Polymers 6077 Non-Phthalate 77 Series Vinyl Compound
Description: The Colorite 77 series is a family of compounds designed for those medical device producers that require the use of a non-phthalate plasticizer that has superior resistance to extractio..
Brittleness Temperature -47.0 °C
-52.6 °F
ASTM D-746
Axiall 10753 Wire & Cable Flexible PVC
Flame retardant 60C compound suitable for integral non-metallic conduit and general purpose jacket applications. Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Brittleness Temperature -47.0 °C
-52.6 °F
ASTM D746
Teknor Apex APEX® 1700-50 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose, Low Gloss Uses-Appliance Components, Footwear, FurnitureForms-PelletsProcessing Met..
Brittleness Temperature -47.0 °C
-52.6 °F
ASTM D746
Teknor Apex APEX® 2565-H Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-Natural Color, OpaqueForms-PelletsProcessin..