Material Notes:
Flame retardant 60C compound suitable for integral non-metallic conduit and general purpose jacket applications. Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.21 - 1.25 g/cc
1.21 - 1.25 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 72 - 78
72 - 78
delayed; ASTM D-2240
Tensile Strength, Yield 17.6 MPa
2550 psi
ASTM D-638
Elongation at Yield 311.3 %
311.3 %
Air Aging: 168 hours @ 100°C; 30 mil slabs; UL 1581
375 %
375 %
ASTM D-638
100% Modulus 0.007412 GPa
1.075 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -47.0 °C
-52.6 °F
ASTM D-746
Oxygen Index 24 %
24 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 182 °C
360 °F