Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eastman M3006-P Polyethylene  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman M3006-P Polyethylene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Medium density polyethylene M3006-P is a specialty formulation suggested for high speed extrusion coating applications. M3006-P offers improvements over low density polyethylene in barrier properties and high temperature resistance.Information supplied by the manufacturer.Information from manufacturer data sheet.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line.
Physical Properties Metric English Comments
Density 0.933 g/cc
0.0337 lb/in³
ASTM D4883
Melt Flow 4.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 16.5 MPa
2390 psi
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Elongation at Break 67 %
67 %
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Flexural Modulus 0.572 GPa
83.0 ksi
2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 100 °C
212 °F
ASTM D1525
Brittleness Temperature -47.0 °C
-52.6 °F
ASTM D746
Descriptive Properties Value Comments
Process Coating