Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Teknor Apex Flexalloy® 9604-75 Polyvinyl Chloride, Elastomer

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade , PVC, Wire and Cable Grade
Manufacturer Teknor Apex Company
Trade Name Flexalloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Flexalloy® 9604-75 Polyvinyl Chloride, Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Notes: 105°C Jacket; RoHS Compliant Features: Flame Retardant; High Heat Resistance; Low Temperature Flexibility; Sunlight Resistant (720 hours) Uses Cable Jacketing Wire Types: SEOW; SEW; SJEOW; SJEW; STEOW; STEW Agency Ratings: UL Class 11; UL Class 12; UL Class 36; UL Class 43; UL QMTT2 .E73402 Forms: PelletsInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
ASTM D792
Melt Flow 7.80 g/10 min

@Load 2.16 kg,
Temperature 230 °C
7.80 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
15 seconds; ASTM D2240
Tensile Strength at Break 16.8 MPa
2440 psi
ASTM D638
Elongation at Break 380 %
380 %
ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 105 °C
221 °F
Continuous Use; ASTM D794
Brittleness Temperature -47.0 °C
-52.6 °F
ASTM D746
Oxygen Index 25 %
25 %
ASTM D2863
Electrical Properties Metric English Comments
Dielectric Constant 3.75

@Frequency 1.00e+6 Hz
3.75

@Frequency 1.00e+6 Hz
ASTM D150
5.56

@Frequency 1000 Hz
5.56

@Frequency 1000 Hz
ASTM D150
Dissipation Factor 0.098

@Frequency 1.00e+6 Hz
0.098

@Frequency 1.00e+6 Hz
ASTM D150
0.14

@Frequency 1000 Hz
0.14

@Frequency 1000 Hz
ASTM D150
Descriptive Properties Value Comments
Appearance Opaque
Users viewing this material also viewed the following: