Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -51.0 - -12.0 °C | -59.8 - 10.4 °F | Average value: -36.5 °C Grade Count:24 |
Overview of materials for Thermoset Polyurethane Foam, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu.. |