Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical without Impact | 115 °C @Thickness 1.50 mm |
239 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources PC-GP1-D Polycarbonate, General Purpose, Low Flow Polycarbonate, General Purpose, Low FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/.. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 3.00 mm |
239 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-GP1-D-[color]-1 Polycarbonate, General Purpose, Low Flow with Mold Release Polycarbonate, General Purpose, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 1.50 mm |
239 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources PC-GP2-D Polycarbonate, General Purpose, Medium Flow Polycarbonate, General Purpose, Medium FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on.. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 3.00 mm |
239 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-GP2-D-[color]-1 Polycarbonate, General Purpose, Medium Flow with Mold Release Polycarbonate, General Purpose, Medium Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf.. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 3.00 mm |
239 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-GP3-D Polycarbonate, General Purpose, High Flow Polycarbonate, General Purpose, High FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inc.. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 3.00 mm |
239 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-GP3-D-[color]-1 Polycarbonate, General Purpose, High Flow with Mold Release Polycarbonate, General Purpose, High Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 1.50 mm |
239 °F @Thickness 0.0591 in |
DAM; UL 746B |
DuPont Performance Polymers Minlon® 10B140 BK061 Nylon 66
(Unverified Data**) Minlon® 10B140 BK061 is a 40% mineral reinforced, black polyamide 66 resin for injection molding. It has very low warpage.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 3.00 mm |
239 °F @Thickness 0.118 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® FR70M30V0 BK010 Nylon 66
(Unverified Data**) Zytel® FR70M30V0 BK010 is a 30% mineral reinforced, flame retardant, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 1.50 mm |
239 °F @Thickness 0.0591 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® FR70M30V0 BK010 Nylon 66
(Unverified Data**) Zytel® FR70M30V0 BK010 is a 30% mineral reinforced, flame retardant, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness >=0.750 mm |
239 °F @Thickness >=0.0295 in |
|
LG Chemical LUMID GP2151BF PA66+GF15%, Flame Retardant Feature: Injection Molding, PA66+GF15%, Halogen Free Flame RetardantApplication: ConnectorsCAS No. 32131-17-2, 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG.. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness >=1.50 mm |
239 °F @Thickness >=0.0591 in |
|
LG Chemical LUMID GP2151BF PA66+GF15%, Flame Retardant Feature: Injection Molding, PA66+GF15%, Halogen Free Flame RetardantApplication: ConnectorsCAS No. 32131-17-2, 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG.. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 0.780 - 1.57 mm |
239 °F @Thickness 0.0307 - 0.0618 in |
UL 746 |
A. Schulman POLYFLAM™ FPP 1007E Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1007E is a 40% talc filled homopolymer compound for extrusion applications.Information provided by A. Schulman. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 0.780 mm |
239 °F @Thickness 0.0307 in |
UL 746 |
A. Schulman POLYFLAM™ FPP 1007 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1007 is a 40% talc filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 0.780 - 1.57 mm |
239 °F @Thickness 0.0307 - 0.0618 in |
UL 746 |
A. Schulman POLYFORT™ FPP 1310 Coupled Mica Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1310 is a Coupled Mica filled homopolymer polypropylene compound for injection molding.Information provided by A. Schulman. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 1.57 mm |
239 °F @Thickness 0.0618 in |
UL 746 |
A. Schulman POLYFLAM™ FPP 1007 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1007 is a 40% talc filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 1.57 mm |
239 °F @Thickness 0.0618 in |
UL 746 |
A. Schulman POLYFLAM™ FPP 1007 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1007 is a 40% talc filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 1.50 mm |
239 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 47H BK0668 Nylon 66, Impact Modified, Heat Stabilized, DAM Vydyne® 47H BK0668 is a high-performance, medium-impact-modified, heat-stabilized grade of PA66 resin.Availability:Asia PacificEuropeNorth AmericaAdditive:Impact Modifier Features:Gasoline Resistan.. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 3.00 mm |
239 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 47H BK0668 Nylon 66, Impact Modified, Heat Stabilized, DAM Vydyne® 47H BK0668 is a high-performance, medium-impact-modified, heat-stabilized grade of PA66 resin.Availability:Asia PacificEuropeNorth AmericaAdditive:Impact Modifier Features:Gasoline Resistan.. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 0.750 mm |
239 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 0.750 mm |
239 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R515 Nylon 66, 15% Glass Reinforced, DAM Vydyne® R515 is general-purpose, 15% glass-fiber reinforced PA66 resin. Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 15% Filler by WeightAdditive:Lubricant Features.. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 0.750 mm |
239 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R540 Nylon 66, 40% Glass Reinforced, DAM Vydyne® R540 is general-purpose, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when.. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 0.750 mm |
239 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® 47 BK11 Nylon 66, Impact Modified, DAM Vydyne® 47H BK11 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 3.00 mm |
239 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 47H BK0644 Nylon 66, Impact Modified, DAM Vydyne® 47H BK0644 is a high-performance, medium-impact-modified, heat-stabilized PA66 resin with excellent UV stability and outstanding processing characteristics. This product has an UL746C f1 ra.. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 0.710 mm |
239 °F @Thickness 0.0280 in |
UL 746 |
Ascend Performance Materials Vydyne® 22HSP Nylon 66, General Purpose, Heat Stabilized, DAM Availability:Asia PacificEuropeNorth America Additive:Lubricant Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood To.. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 0.750 mm |
239 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® 47H BK03 Nylon 66, Impact Modified, DAM Vydyne® 47H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 1.50 mm |
239 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 47H BK03 Nylon 66, Impact Modified, DAM Vydyne® 47H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 3.00 mm |
239 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 47H BK03 Nylon 66, Impact Modified, DAM Vydyne® 47H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 0.750 mm |
239 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R530 NAT Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530 NAT is general-purpose, injection-molding grade, 30% glass-fiber reinforced PA66 resin. Available in natural, it is lubricated for good machine feed, flow and mold releaseAvailability:.. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 1.57 mm |
239 °F @Thickness 0.0618 in |
UL 746 |
A. Schulman POLYFLAM™ FPP 1007 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1007 is a 40% talc filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 0.780 mm |
239 °F @Thickness 0.0307 in |
UL 746 |
A. Schulman POLYFLAM™ FPP 1007 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1007 is a 40% talc filled homopolymer polypropylene compound.Information provided by A. Schulman. |