Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Zytel® FR70M30V0 BK010 Nylon 66  (Unverified Data**)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Mineral Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Zytel® FR70M30V0 BK010 Nylon 66  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Zytel® FR70M30V0 BK010 is a 30% mineral reinforced, flame retardant, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.62 g/cc
0.0585 lb/in³
DAM; ISO 1183
Filler Content 30 %
30 %
DAM
Linear Mold Shrinkage, Flow 0.0080 cm/cm

@Thickness 2.00 mm
0.0080 in/in

@Thickness 0.0787 in
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0090 cm/cm

@Thickness 2.00 mm
0.0090 in/in

@Thickness 0.0787 in
DAM; ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 45.0 MPa

@Temperature 23.0 °C
6530 psi

@Temperature 73.4 °F
50%RH; ISO 527
65.0 MPa

@Temperature 23.0 °C
9430 psi

@Temperature 73.4 °F
DAM; ISO 527
Elongation at Break 2.0 %

@Temperature 23.0 °C
2.0 %

@Temperature 73.4 °F
DAM; ISO 527
3.5 %

@Temperature 23.0 °C
3.5 %

@Temperature 73.4 °F
50%RH; ISO 527
Tensile Modulus 4.00 GPa

@Temperature 23.0 °C
580 ksi

@Temperature 73.4 °F
50%RH; ISO 527
6.20 GPa

@Temperature 23.0 °C
899 ksi

@Temperature 73.4 °F
DAM; ISO 527
Izod Impact, Notched (ISO) 2.00 kJ/m²

@Temperature 23.0 °C
0.952 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 180/1A
2.50 kJ/m²

@Temperature 23.0 °C
1.19 ft-lb/in²

@Temperature 73.4 °F
50%RH; ISO 180/1A
Charpy Impact Unnotched 2.00 J/cm²

@Temperature 23.0 °C
9.52 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eU
2.50 J/cm²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
50%RH; ISO 179/1eU
Charpy Impact, Notched 0.250 J/cm²

@Temperature 23.0 °C
1.19 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eA
0.250 J/cm²

@Temperature 23.0 °C
1.19 ft-lb/in²

@Temperature 73.4 °F
50%RH; ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 263 °C
505 °F
10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 145 °C
293 °F
DAM; ISO 75-1/-2
UL RTI, Electrical 105 °C

@Thickness 0.750 mm
221 °F

@Thickness 0.0295 in
DAM; UL 746B
105 °C

@Thickness 1.00 mm
221 °F

@Thickness 0.0394 in
DAM; UL 746B
120 °C

@Thickness 3.00 mm
248 °F

@Thickness 0.118 in
DAM; UL 746B
120 °C

@Thickness 1.50 mm
248 °F

@Thickness 0.0591 in
DAM; UL 746B
UL RTI, Mechanical with Impact 95.0 °C

@Thickness 1.00 mm
203 °F

@Thickness 0.0394 in
DAM; UL 746B
95.0 °C

@Thickness 0.750 mm
203 °F

@Thickness 0.0295 in
DAM; UL 746B
105 °C

@Thickness 1.50 mm
221 °F

@Thickness 0.0591 in
DAM; UL 746B
115 °C

@Thickness 3.00 mm
239 °F

@Thickness 0.118 in
DAM; UL 746B
UL RTI, Mechanical without Impact 105 °C

@Thickness 1.00 mm
221 °F

@Thickness 0.0394 in
DAM; UL 746B
105 °C

@Thickness 0.750 mm
221 °F

@Thickness 0.0295 in
DAM; UL 746B
115 °C

@Thickness 3.00 mm
239 °F

@Thickness 0.118 in
DAM; UL 746B
115 °C

@Thickness 1.50 mm
239 °F

@Thickness 0.0591 in
DAM; UL 746B
Flammability, UL94 V-2

@Thickness 0.750 mm
V-2

@Thickness 0.0295 in
DAM; IEC 60695-11-10
V-2

@Thickness 0.750 mm
V-2

@Thickness 0.0295 in
DAM; UL94
V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
DAM; IEC 60695-11-10
V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
DAM; IEC 60695-11-10
V-0

@Thickness 1.00 mm
V-0

@Thickness 0.0394 in
DAM; IEC 60695-11-10
V-0

@Thickness 1.00 mm
V-0

@Thickness 0.0394 in
DAM; UL94
V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
DAM; UL94
V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
DAM; UL94
5VA

@Thickness 1.50 mm
5VA

@Thickness 0.0591 in
DAM; IEC 60695-11-20
Glow Wire Test 800 °C

@Thickness 1.50 mm
1470 °F

@Thickness 0.0591 in
DAM; Ignition; IEC 60695-2-13
800 °C

@Thickness 1.00 mm
1470 °F

@Thickness 0.0394 in
DAM; Ignition; IEC 60695-2-13
800 °C

@Thickness 3.00 mm
1470 °F

@Thickness 0.118 in
DAM; Ignition; IEC 60695-2-13
800 °C

@Thickness 0.750 mm
1470 °F

@Thickness 0.0295 in
DAM; Ignition; IEC 60695-2-13
960 °C

@Thickness 1.50 mm
1760 °F

@Thickness 0.0591 in
DAM; IEC 60695-2-12
960 °C

@Thickness 3.00 mm
1760 °F

@Thickness 0.118 in
DAM; IEC 60695-2-12
960 °C

@Thickness 1.00 mm
1760 °F

@Thickness 0.0394 in
DAM; IEC 60695-2-12
960 °C

@Thickness 0.750 mm
1760 °F

@Thickness 0.0295 in
DAM; IEC 60695-2-12
Electrical Properties Metric English Comments
Comparative Tracking Index 250 - 400 V

@Thickness 1.50 mm
250 - 400 V

@Thickness 0.0591 in
DAM; UL 746A
250 - 400 V

@Thickness 0.750 mm
250 - 400 V

@Thickness 0.0295 in
DAM; UL 746A
250 - 400 V

@Thickness 3.00 mm,
Temperature 23.0 °C
250 - 400 V

@Thickness 0.118 in,
Temperature 73.4 °F
DAM; UL 746A
250 - 400 V

@Thickness 1.00 mm,
Temperature 23.0 °C
250 - 400 V

@Thickness 0.0394 in,
Temperature 73.4 °F
DAM; UL 746A
Processing Properties Metric English Comments
Melt Temperature 290 °C
554 °F
DAM; Optimum
280 - 300 °C
536 - 572 °F
DAM
Mold Temperature 90.0 °C
194 °F
DAM; optimum
70.0 - 110 °C
158 - 230 °F
DAM
Drying Temperature 80.0 °C
176 °F
DAM
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
DAM
Moisture Content <= 0.20 %
<= 0.20 %
DAM
Descriptive Properties Value Comments
Additive Flame Retardant
DAM
Appearance Black Color
DAM
Drying Recommended Yes, if moisture content of resin exceeds recommended level
DAM
Features Chemical Resistance, Good
DAM
Flame Retardant
DAM
Filler Mineral filler
DAM
Forms Pellets
DAM
Generic Nylon 66
DAM
Material Status Current
DAM
Part Marking Code >PA66-MD30FR(17)<
ISO 11469; DAM
Polymer Family Polyamide
DAM
Polymer Type PA66
DAM
Processing Method Injection Molding
DAM
Product Category Flame Retardant Resins
DAM
Low Warp Resins
DAM
Mineral Reinforced Resins
DAM
Region Available - Global Yes
DAM
Resin Identification PA66-MD30FR(17)
ISO 1043; DAM
RoHS Compliance Contact Manufacturer
DAM
Uses Appliance Components
DAM
Automotive Applications
DAM
Connectors
DAM
Electrical/Electronic Applications
DAM
Industrial Applications
DAM