Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Electrical | 75.0 °C @Thickness 1.50 mm |
167 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources PC/TP-GP2 PC/Polyester Alloy High Impact, Excellent Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided b.. |
|||
UL RTI, Electrical | 75.0 °C @Thickness 3.00 mm |
167 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC/TP-GP2 PC/Polyester Alloy High Impact, Excellent Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided b.. |
|||
UL RTI, Electrical | 75.0 °C @Thickness 0.749 mm |
167 °F @Thickness 0.0295 in |
UL 746 |
Polymer Resources TP-FR-IM2 Polybutylene Terephthalate, Impact Modified, Flame Retardant, High Flow Polybutylene Terephthalate, Impact Modified, Flame Retardant, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
UL RTI, Electrical | 75.0 °C @Thickness 1.50 mm |
167 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources TP-FR-IM2 Polybutylene Terephthalate, Impact Modified, Flame Retardant, High Flow Polybutylene Terephthalate, Impact Modified, Flame Retardant, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
UL RTI, Electrical | 75.0 °C @Thickness 3.00 mm |
167 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources TP-FR-IM2 Polybutylene Terephthalate, Impact Modified, Flame Retardant, High Flow Polybutylene Terephthalate, Impact Modified, Flame Retardant, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
UL RTI, Electrical | 75.0 °C @Thickness 1.50 mm |
167 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources TP-G30 Polybutylene Terephthalate, 30% Glass Reinforced Polybutylene Terephthalate, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
UL RTI, Electrical | 75.0 °C @Thickness 3.00 mm |
167 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources TP-G30 Polybutylene Terephthalate, 30% Glass Reinforced Polybutylene Terephthalate, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
UL RTI, Electrical | 75.0 °C @Thickness 1.50 mm |
167 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources TP-IGFR-G30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant, Reduced Warpage Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant, Reduced WarpageProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmen.. |
|||
UL RTI, Electrical | 75.0 °C @Thickness 3.00 mm |
167 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources TP-IGFR-G30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant, Reduced Warpage Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant, Reduced WarpageProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmen.. |
|||
UL RTI, Electrical | 75.0 °C @Thickness >=2.10 mm |
167 °F @Thickness >=0.0827 in |
|
LG Chemical AF312B ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
UL RTI, Electrical | 75.0 °C @Thickness >=2.50 mm |
167 °F @Thickness >=0.0984 in |
|
LG Chemical AF312B ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
UL RTI, Electrical | 75.0 °C @Thickness >=3.00 mm |
167 °F @Thickness >=0.118 in |
|
LG Chemical AF312B ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
UL RTI, Electrical | 75.0 °C @Thickness >=0.550 mm |
167 °F @Thickness >=0.0217 in |
|
LG Chemical Lupox® GP1006FD PBT Description: Injection Molding, PBT, Flame Retardant, High ImpactApplication: IT/OA, Automotive (Connector)CAS No. 68928-70-1, 155123-66-3, 24968-12-5 and 1309-64-4Information provided by LG Chemica.. |
|||
UL RTI, Electrical | 75.0 °C @Thickness >=0.800 mm |
167 °F @Thickness >=0.0315 in |
|
LG Chemical Lupox® GP2400G PBT+GF40% Description: Injection Molding, PBT+GF40%, HCFC ResistantApplication: E&E (Muffler of Refrigerator)CAS No. 65997-17-3 and 30965-26-5Information provided by LG Chemical |
|||
UL RTI, Electrical | 75.0 °C @Thickness >=3.00 mm |
167 °F @Thickness >=0.118 in |
|
LG Chemical Lupox® GP2400G PBT+GF40% Description: Injection Molding, PBT+GF40%, HCFC ResistantApplication: E&E (Muffler of Refrigerator)CAS No. 65997-17-3 and 30965-26-5Information provided by LG Chemical |
|||
UL RTI, Electrical | 75.0 °C @Thickness >=0.800 mm |
167 °F @Thickness >=0.0315 in |
|
LG Chemical Lupox® NH2306F PBT+GF30% Description: Injection Molding, PBT+GF30%, Halogen Free Flame RetardantApplication: IT/OA, E&E (Connector)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
UL RTI, Electrical | 75.0 °C @Thickness >=1.60 mm |
167 °F @Thickness >=0.0630 in |
|
LG Chemical Lupox® NH2306F PBT+GF30% Description: Injection Molding, PBT+GF30%, Halogen Free Flame RetardantApplication: IT/OA, E&E (Connector)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
UL RTI, Electrical | 75.0 °C @Thickness >=3.20 mm |
167 °F @Thickness >=0.126 in |
|
LG Chemical Lupox® NH2306F PBT+GF30% Description: Injection Molding, PBT+GF30%, Halogen Free Flame RetardantApplication: IT/OA, E&E (Connector)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
UL RTI, Electrical | 75.0 °C @Thickness >=0.500 mm |
167 °F @Thickness >=0.0197 in |
|
LG Chemical Lupox® TE5006F PET+PC Description: Injection Molding, PET+PC, Flame Retardant, GWIT, CTIApplication: IT/OA, E&E (Connector)CAS No. 68928-70-1, 103598-77-2, 25038-59-9 and 1309-64-4Information provided by LG Chemical |
|||
UL RTI, Electrical | 75.0 °C @Thickness 0.930 mm |
167 °F @Thickness 0.0366 in |
UL746B |
DSM Arnite® A06 101 PET (European Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
UL RTI, Electrical | 75.0 °C @Thickness 3.00 mm |
167 °F @Thickness 0.118 in |
UL746B |
DSM Arnite® A06 101 PET (European Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
UL RTI, Electrical | 75.0 °C @Thickness 1.50 mm |
167 °F @Thickness 0.0591 in |
UL746B |
DSM Arnite® A04 900 PET (European Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
UL RTI, Electrical | 75.0 °C @Thickness 0.750 mm |
167 °F @Thickness 0.0295 in |
UL746B |
DSM Arnite® A04 900 PET (European Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
UL RTI, Electrical | 75.0 °C @Thickness 0.750 mm |
167 °F @Thickness 0.0295 in |
UL746B |
DSM Arnite® T06 204 SN PBT (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
UL RTI, Electrical | 75.0 °C @Thickness 3.00 mm |
167 °F @Thickness 0.118 in |
UL746B |
DSM Arnite® T06 204 SN PBT (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |