Thermal Properties Metric English Comments
UL RTI, Mechanical without Impact 75.0 - 130 °C
167 - 266 °F
Average value: 107 °C Grade Count:8
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re..
UL RTI, Mechanical without Impact 50.0 - 130 °C
122 - 266 °F
Average value: 92.0 °C Grade Count:14
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi..
UL RTI, Mechanical without Impact 125 - 130 °C
257 - 266 °F
Average value: 126 °C Grade Count:4
Overview of materials for Polycarbonate, Gamma Radiation Resistant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum..
UL RTI, Mechanical without Impact 80.0 - 130 °C
176 - 266 °F
Average value: 107 °C Grade Count:13
Overview of materials for Polycarbonate, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E..
UL RTI, Mechanical without Impact 110 - 130 °C
230 - 266 °F
Average value: 122 °C Grade Count:16
Overview of materials for Nylon 46, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values ..
UL RTI, Mechanical without Impact 50.0 - 130 °C
122 - 266 °F
Average value: 119 °C Grade Count:3
Overview of materials for Polyimide, Graphite Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Graphite Filled". Each property range of values reported is minimum and maximum values of app..