Material Notes:
Product Description: A high crystallinity, high impact copolymer resin designed for injection molded applications requiring excellent processing attributes.Availability: North America Features:Balanced Stiffness/ToughnessGood Heat Aging ResistanceGood Impact ResistanceGood ProcessabilityMedium Molecular Weight Nucleated Processing Method: Blow Molding, Compound and Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ExxonMobil Method
Melt Flow 16 g/10 min

@Load 2.16 kg,
Temperature 230 °C
16 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.2 MPa
2780 psi
2.0 in/min; ASTM D638
Elongation at Yield 7.0 %
7.0 %
2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 938 MPa
136000 psi
0.05 in/min; ASTM D790A
1080 MPa
156000 psi
0.5 in/min; ASTM D790B
Izod Impact, Notched NB
NB
ASTM D256A
Impact Test 39.7 J

@Thickness 3.17 mm,
Temperature -28.9 °C
29.3 ft-lb

@Thickness 0.125 in,
Temperature -20.0 °F
ASTM D3763
46.4 J

@Thickness 3.17 mm,
Temperature -40.0 °C
34.2 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 87.2 °C
189 °F
ASTM D648