Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 - 210 °C | 181 - 410 °F | Average value: 160 °C Grade Count:22 |
Overview of materials for Nylon 612, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 - 210 °C | 392 - 410 °F | ASTM D1525, HDT Method B |
Loxim 210 01HB Polybutylene Terephthalate Information provided by Loxim Industries |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 207 - 210 °C | 405 - 410 °F | Average value: 208 °C Grade Count:4 |
Overview of materials for Polyethersulfone, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximu.. |