Loxim 210 01HB Polybutylene Terephthalate

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
Manufacturer Loxim Industries
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Loxim 210 01HB Polybutylene Terephthalate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Loxim Industries
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
ASTM D792
Filler Content 10 %
10 %
Linear Mold Shrinkage 0.0060 - 0.010 cm/cm
0.0060 - 0.010 in/in
ASTM D1299
Mechanical Properties Metric English Comments
Tensile Strength at Break 60.0 MPa
8700 psi
ASTM D683
Elongation at Break 3.0 %
3.0 %
ASTM D638
Tensile Modulus 3.50 GPa
508 ksi
ASTM D638
Flexural Modulus 3.00 GPa
435 ksi
ASTM D790
Izod Impact, Notched 0.400 J/cm
0.749 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 200 - 210 °C
392 - 410 °F
ASTM D1525, HDT Method B
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in