Deflection Temperature at 0.46 MPa (66 psi) 90.0 - 170 °C
194 - 338 °F
Average value: 144 °C Grade Count:21
Overview of materials for Polybutylene Terephthalate (PBT), Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Extrusion Grade". Each property range of values reported is minimum an..
Deflection Temperature at 0.46 MPa (66 psi) 75.0 - 170 °C
167 - 338 °F
Average value: 122 °C Grade Count:17
Overview of materials for Cyclo Olefin Polymer
This property data is a summary of similar materials in the MatWeb database for the category "Cyclo Olefin Polymer". Each property range of values reported is minimum and maximum values of appropria..
Deflection Temperature at 0.46 MPa (66 psi) 51.0 - 170 °C
124 - 338 °F
Average value: 119 °C Grade Count:13
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyester Grade". Each property range of values reported is minimum a..
Deflection Temperature at 0.46 MPa (66 psi) 104 - 170 °C
220 - 338 °F
Average value: 133 °C Grade Count:22
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi..