Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 248 °C

@Thickness 3.20 mm
478 °F

@Thickness 0.126 in
unannealed; ASTM D648
Ovation Polymers Opnyl OP66GF15 Nylon 66, 14% Glass Reinforced
Nylon 66 - Glass reinforced (14 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared..
Deflection Temperature at 0.46 MPa (66 psi) 248 °C
478 °F
ISO 75, ASTM D648
Nilit Nilamid A G5 FR PH2 25% Glass Fiber Reinforced, Flame Retardant PA66 (with Red Phosphorous)
Description: Nilamid A G5 FR PH2 combines flame retardancy with outstanding mechanical performance. This product has a complete yellow card, with RTI and CTI listings. The formulation has been optim..
Deflection Temperature at 0.46 MPa (66 psi) 248 °C
478 °F
ASTM D648
Mitsui AURUM® JCL3030 Polyimide, Carbon Fiber Filled  (discontinued **)
AURUM JCL3030 is a high-performance polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, carbon fiber reinforced AU..
Deflection Temperature at 0.46 MPa (66 psi) 248 °C
478 °F
ASTM D648
Mitsui AURUM® JCN3030 Polyimide, Carbon Fiber Filled  (discontinued **)
AURUM JCN3030 is a high-performance polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, carbon fiber reinforced AU..
Deflection Temperature at 0.46 MPa (66 psi) 248 °C

@Thickness 3.20 mm
478 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP LUBRICOMP RAL22 PA 66
LNP LUBRICOMP* RAL22 is a compound based on Nylon 66 resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant.
Deflection Temperature at 0.46 MPa (66 psi) 248 °C

@Thickness 3.20 mm
478 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP LUBRICOMP RAL22 PA 66 (Asia Pacific)
LNP LUBRICOMP* RAL22 is a compound based on Nylon 66 resin containing Aramid, PTFE. Added features of this material include: Internally Lubricated.
Deflection Temperature at 0.46 MPa (66 psi) 248 °C

@Thickness 3.20 mm
478 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP LUBRICOMP RAL22S PA 66
LNP* LUBRICOMP* RAL22S is a compound based on Nylon 66 resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant.
Deflection Temperature at 0.46 MPa (66 psi) 248 °C

@Thickness 3.20 mm
478 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP LUBRICOMP RAL22S PA 66 (Asia Pacific)
LNP* Lubricomp* RAL22S is a compound based on Nylon 66 resin containing PTFE, Aramid Fiber. Added features of this material include: Internally Lubricated.
Deflection Temperature at 0.46 MPa (66 psi) 248 °C

@Thickness 3.20 mm
478 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP 2X98703 ETFE
LNP* THERMOCOMP* 2X98703 is a compound based on ETFE Copolymer resin containint Proprietary Filler(s).
Deflection Temperature at 0.46 MPa (66 psi) 248 °C
478 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP THERMOCOMP RF003H PA 66
LNP* THERMOCOMP* RF003H is a compound based on Nylon 66 containing 15% Glass Fiber. Added feature of this grade is: Healthcare.
Deflection Temperature at 0.46 MPa (66 psi) 248 °C
478 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP THERMOCOMP RF003XXH PA 66
LNP* THERMOCOMP* RF003XXH is a compound based on Nylon 66 containing 15% Glass Fiber. Added feature of this grade is: Healthcare.
Deflection Temperature at 0.46 MPa (66 psi) 248 °C
478 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP THERMOTUF VF004S SUPER TOUGH NYLON (Europe-Africa-Middle East)
LNP* THERMOTUF* VF004S is a compound based on Super Tough Nylon resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
Deflection Temperature at 0.46 MPa (66 psi) 248 °C

@Thickness 3.20 mm
478 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP 2F005 ETFE
LNP* Thermocomp* 2F005 is a fluoropolymer compound based on ETFE containing 25% Glass Fiber.
Deflection Temperature at 0.46 MPa (66 psi) 248 °C
478 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP THERMOCOMP RF006EUC PA 66
LNP* THERMOCOMP* RF006EUC is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include Easy Molding, UV Stabilized.
Deflection Temperature at 0.46 MPa (66 psi) 248 °C
478 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP THERMOCOMP RFM-3353 EM PA 66 (Europe-Africa-Middle East)
LNP* Lubricomp* RFM-3353 EM is a compound based on Nylon 66 resin containing Glass Fiber, Mineral. Added features of this material include: Easy Molding.
Deflection Temperature at 0.46 MPa (66 psi) 248 °C
478 °F
ASTM D648
A. Schulman SCHULAMID® 66 GF13 13% Glass Fiber Reinforced Nylon 66
Information provided by A. Schulman.
Deflection Temperature at 0.46 MPa (66 psi) 248 °C
478 °F
ASTM D648
A. Schulman SCHULAMID® 66 GF13 13% Glass Fiber Reinforced Nylon 66
Information provided by A. Schulman.
Deflection Temperature at 0.46 MPa (66 psi) 248 °C
478 °F
ASTM D648
A. Schulman SCHULAMID® 66 GF13 13% Glass Fiber Reinforced Nylon 66
Information provided by A. Schulman.
Deflection Temperature at 0.46 MPa (66 psi) 248 °C
478 °F
ASTM D648
A. Schulman SCHULAMID® 66 GF13 13% Glass Fiber Reinforced Nylon 66
Information provided by A. Schulman.
Deflection Temperature at 0.46 MPa (66 psi) 248 °C
478 °F
ASTM D648
A. Schulman SCHULAMID® 66 GF13 13% Glass Fiber Reinforced Nylon 66
Information provided by A. Schulman.
Deflection Temperature at 0.46 MPa (66 psi) 248 °C
478 °F
ASTM D648
A. Schulman SCHULAMID® 66 GF13 13% Glass Fiber Reinforced Nylon 66
Information provided by A. Schulman.
Deflection Temperature at 0.46 MPa (66 psi) 248 °C
478 °F
ASTM D648
A. Schulman ComAlloy Comtuf® 635 Nylon 6/6, Glass/Mineral Reinforced, Impact Modified, Flow Enhanced
Data provided by the manufacturer, ComAlloy International Company.40% Glass/Mineral Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has ..
Deflection Temperature at 0.46 MPa (66 psi) 248 °C
478 °F
ASTM D648
A. Schulman ComAlloy Voloy® 430 Glass Reinforced, PBT Alloy, Flame Retardant, UL
Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.