SABIC Innovative Plastics LNP LUBRICOMP RAL22S PA 66

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP RAL22S PA 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* LUBRICOMP* RAL22S is a compound based on Nylon 66 resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ASTM D792
1.22 g/cc
0.0441 lb/in³
ISO 1183
Moisture Absorption 0.700 %
0.700 %
50% RH, 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.019 cm/cm

@Time 86400 sec
0.019 in/in

@Time 24.0 hour
ASTM D955
0.0192 cm/cm

@Time 86400 sec
0.0192 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.0195 cm/cm

@Time 86400 sec
0.0195 in/in

@Time 24.0 hour
ISO 294
0.020 cm/cm

@Time 86400 sec
0.020 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 79.0 MPa
11500 psi
ISO 527
81.0 MPa
11700 psi
ASTM D638
Elongation at Break 8.1 %
8.1 %
ASTM D638
9.5 %
9.5 %
ISO 527
Tensile Modulus 3.44 GPa
499 ksi
50 mm/min; ASTM D638
3.50 GPa
508 ksi
1 mm/min; ISO 527
Flexural Strength 110 MPa
16000 psi
ASTM D790
117 MPa
17000 psi
ISO 178
Flexural Modulus 2.96 GPa
429 ksi
ASTM D790
3.50 GPa
508 ksi
ISO 178
Izod Impact, Notched 1.33 J/cm
2.49 ft-lb/in
ASTM D256
Izod Impact, Unnotched 7.47 J/cm
14.0 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 48.0 kJ/m²
22.8 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 6.00 J
4.43 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Impact Test 1.00 J
0.738 ft-lb
Multiaxial Impact; ISO 6603
Coefficient of Friction, Dynamic 0.55
0.55
ASTM D3702 Modified
Coefficient of Friction, Static 0.46
0.46
ASTM D3702 Modified
K (wear) Factor 26.2 x 10-8 mm³/N-M
13.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 73.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
40.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
73.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
CTE, linear, Transverse to Flow 82.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
45.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
82.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 248 °C

@Thickness 3.20 mm
478 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 193 °C
379 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
198 °C

@Thickness 3.20 mm
388 °F

@Thickness 0.126 in
unannealed; ASTM D648