Techmer ES HiFill® ABS IM TM20 20% Mineral Filled

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer Techmer ES
Trade Name HiFill®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® ABS IM TM20 20% Mineral Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 20% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Water Absorption 0.13 %

@Time 86400 sec
0.13 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0015 cm/cm

@Thickness 3.17 mm
0.0015 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 107
107
ASTM D785
Tensile Strength 73.1 MPa
10600 psi
ASTM D638
Elongation at Yield 3.5 %
3.5 %
ASTM D638
Flexural Yield Strength 109 MPa
15800 psi
ASTM D790
Flexural Modulus 3.93 GPa
570 ksi
ASTM D790
Izod Impact, Notched 1.01 J/cm

@Thickness 3.17 mm
1.90 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 5.07 J/cm

@Thickness 3.17 mm
9.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 34.2 µm/m-°C
19.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 112 °C
233 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 103 °C
218 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Strength 17.7 kV/mm
450 kV/in
Method A (Short-Time); ASTM D149