Material Notes:
Product Description: A high crystallinity, medium impact copolymer resin designed for injection-molded automotive interior applications and large appliance parts applications requiring high melt flow rate and excellent processing attributes.Availability: North America Features:Fast Molding CycleGood FlowGood StiffnessImpact ModifiedNucleatedUses: AppliancesAutomotive ApplicationsAutomotive Interior PartsCompoundingConsumer ApplicationsIndustrial ApplicationsProcessing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ExxonMobil Method
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.2 MPa
3650 psi
2.0 in/min; ASTM D638
Elongation at Yield 4.7 %
4.7 %
2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 1350 MPa
196000 psi
0.05 in/min; ASTM D790A
1530 MPa
222000 psi
0.5 in/min; ASTM D790B
Izod Impact, Notched 0.854 J/cm
1.60 ft-lb/in
ASTM D256A
Gardner Impact 21.5 J

@Thickness 3.17 mm,
Temperature -28.9 °C
15.8 ft-lb

@Thickness 0.125 in,
Temperature -20.0 °F
Geometry GC; ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 108 °C
227 °F
ASTM D648