Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 - 100 °C | 194 - 212 °F | ISO 75-2 |
Prodways PLASTCure Model 200 3D Printing Polymer High temperature resistance.Thermoforming applicationsInformation provided by Genistar. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 82.8 - 100 °C | 181 - 212 °F | Average value: 94.2 °C Grade Count:37 |
Overview of materials for Polystyrene, Heat Resistant Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.0 - 100 °C | 190 - 212 °F | Average value: 94.8 °C Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled". Each property range of values reported is m.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 - 100 °C | 176 - 212 °F | Average value: 92.0 °C Grade Count:12 |
Overview of materials for Ethylene Vinyl Alcohol (EVOH) This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Alcohol". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 - 100 °C | 194 - 212 °F | ASTM D1525, HDT Method B |
Loxim 800 00 HB Polypropylene Compound, Flame Retardant Information provided by Loxim Industries |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 95.0 - 100 °C | 203 - 212 °F | |
C.O.I.M. EXTER S® S 107 Orthophthalic Resin Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 107: Resin for trans.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 84.0 - 100 °C | 183 - 212 °F | Average value: 94.7 °C Grade Count:3 |
Overview of materials for Polystyrene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 - 100 °C | 169 - 212 °F | Average value: 85.1 °C Grade Count:9 |
Overview of materials for Styrene/Methyl Methacrylate Copolymer (SMMA) This property data is a summary of similar materials in the MatWeb database for the category "Styrene/Methyl Methacrylate Copolymer (SMMA)". Each property range of values reported is minimum and max.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 - 100 °C | 117 - 212 °F | Average value: 77.4 °C Grade Count:7 |
Overview of materials for Thermoset Polyurethane Foam, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu.. |