Material Notes:
Information provided by Loxim Industries
Physical Properties Metric English Comments
Specific Gravity 0.850 - 0.950 g/cc
0.850 - 0.950 g/cc
ASTM D792
Linear Mold Shrinkage 0.017 - 0.023 cm/cm
0.017 - 0.023 in/in
ASTM D1299
Mechanical Properties Metric English Comments
Tensile Strength at Break 34.0 - 36.0 MPa
4930 - 5220 psi
ASTM D683
Flexural Modulus 1.30 - 1.50 GPa
189 - 218 ksi
ASTM D790
Izod Impact, Notched 0.300 - 0.400 J/cm
0.562 - 0.749 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 - 100 °C
194 - 212 °F
ASTM D1525, HDT Method B
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in