Thermal Properties Metric English Comments
CTE, linear 17.73 µm/m-°C

@Temperature 25.0 - 250 °C
9.850 µin/in-°F

@Temperature 77.0 - 482 °F
Carpenter Gall-Tough® Stainless
Data provided by Carpenter Technology Corporation.6.4 mm diameter tensile specimens from center of 25.4 mm diameter bar annealed 1066°C 1 hour, water quenched, and ground.Threshold Galling Stress 1..
CTE, linear 17.73 µm/m-°C

@Temperature 25.0 - 250 °C
9.850 µin/in-°F

@Temperature 77.0 - 482 °F
Carpenter Gall-Tough® Stainless, Annealed and Cold Drawn Bar, 20% Cold Work
Data provided by Carpenter Technology Corporation.Threshold Galling Stress 103 MPa (higher stress tests not performed). The avg. total volume loss on the wear test is 5 mm³ at 100 rpm.Gall-Tough®..
CTE, linear 17.73 µm/m-°C

@Temperature 25.0 - 250 °C
9.850 µin/in-°F

@Temperature 77.0 - 482 °F
Carpenter Gall-Tough® Stainless, Annealed and Cold Drawn Bar, 10% Cold Work
Data provided by Carpenter Technology Corporation.Threshold Galling Stress 103 MPa (higher stress tests not performed). The avg. total volume loss on the wear test is 5 mm³ at 100 rpm.Gall-Tough®..
CTE, linear 17.73 µm/m-°C

@Temperature 25.0 - 250 °C
9.850 µin/in-°F

@Temperature 77.0 - 482 °F
Carpenter Gall-Tough® Stainless, Annealed and Cold Drawn Bar, 0% Cold Work
Data provided by Carpenter Technology Corporation.Threshold Galling Stress 103 MPa (higher stress tests not performed). The avg. total volume loss on the wear test is 5 mm³ at 100 rpm.Gall-Tough®..