Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 17.73 µm/m-°C @Temperature 25.0 - 250 °C |
9.850 µin/in-°F @Temperature 77.0 - 482 °F |
|
Carpenter Gall-Tough® Stainless Data provided by Carpenter Technology Corporation.6.4 mm diameter tensile specimens from center of 25.4 mm diameter bar annealed 1066°C 1 hour, water quenched, and ground.Threshold Galling Stress 1.. |
|||
CTE, linear | 17.73 µm/m-°C @Temperature 25.0 - 250 °C |
9.850 µin/in-°F @Temperature 77.0 - 482 °F |
|
Carpenter Gall-Tough® Stainless, Annealed and Cold Drawn Bar, 20% Cold Work Data provided by Carpenter Technology Corporation.Threshold Galling Stress 103 MPa (higher stress tests not performed). The avg. total volume loss on the wear test is 5 mm³ at 100 rpm.Gall-Tough®.. |
|||
CTE, linear | 17.73 µm/m-°C @Temperature 25.0 - 250 °C |
9.850 µin/in-°F @Temperature 77.0 - 482 °F |
|
Carpenter Gall-Tough® Stainless, Annealed and Cold Drawn Bar, 10% Cold Work Data provided by Carpenter Technology Corporation.Threshold Galling Stress 103 MPa (higher stress tests not performed). The avg. total volume loss on the wear test is 5 mm³ at 100 rpm.Gall-Tough®.. |
|||
CTE, linear | 17.73 µm/m-°C @Temperature 25.0 - 250 °C |
9.850 µin/in-°F @Temperature 77.0 - 482 °F |
|
Carpenter Gall-Tough® Stainless, Annealed and Cold Drawn Bar, 0% Cold Work Data provided by Carpenter Technology Corporation.Threshold Galling Stress 103 MPa (higher stress tests not performed). The avg. total volume loss on the wear test is 5 mm³ at 100 rpm.Gall-Tough®.. |