Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 7.20 µm/m-°C @Temperature 204 °C |
4.00 µin/in-°F @Temperature 400 °F |
with ply; 8HS form; ASTM D696 |
Park Electrochemical Nelcote® F-555 Phenolic Prepreg, ENKA Reinforced Nelcote® F-555 is a carbon-filled MIL-R-9299 phenolic resin optimized for coating Carbonized Rayon cloth. F-555 is used extensively in the manufacture of high temperature rocket nozzles, heat shiel.. |
|||
CTE, linear | 7.20 µm/m-°C @Temperature 204 °C |
4.00 µin/in-°F @Temperature 400 °F |
with ply; 8HS form; ASTM D696 |
Park Electrochemical Nelcote® F-555 Phenolic Prepreg, NARC/CYDSA Reinforced Nelcote® F-555 is a carbon-filled MIL-R-9299 phenolic resin optimized for coating Carbonized Rayon cloth. F-555 is used extensively in the manufacture of high temperature rocket nozzles, heat shiel.. |
|||
CTE, linear | 7.20 µm/m-°C @Temperature 20.0 - 100 °C |
4.00 µin/in-°F @Temperature 68.0 - 212 °F |
|
H.C. Starck WCu 85/15 Tungsten-Copper Composite Material Description of Product: Tungsten-copper composite materials are produced by copper infiltration of porous sintered tungsten. They are available with different copper contents (10 - 30 %). A therm.. |
|||
CTE, linear | 7.20 µm/m-°C @Temperature 20.0 - 300 °C |
4.00 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott BG36 Band Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include BC20 |
|||
CTE, linear | 7.20 µm/m-°C @Temperature 20.0 - 300 °C |
4.00 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott NG1 Neutral Density Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include NG3, NG4, NG5, NG9, NG10, NG11, NG 12 |
|||
CTE, linear | 7.20 µm/m-°C @Temperature 20.0 - 300 °C |
4.00 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott NG10 Neutral Density Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include NG3, NG4, NG5, NG9, NG1, NG11, NG 12 |
|||
CTE, linear | 7.20 µm/m-°C @Temperature 20.0 - 300 °C |
4.00 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott NG4 Neutral Density Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include NG3, NG1, NG5, NG9, NG10, NG11, NG 12 |
|||
CTE, linear | 7.20 µm/m-°C @Temperature 20.0 - 300 °C |
4.00 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-LASF46A Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 7.20 µm/m-°C @Temperature -30.0 - 70.0 °C |
4.00 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-SSK8 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 7.20 µm/m-°C @Temperature -30.0 - 70.0 °C |
4.00 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott P-SK57 Glass Suitable for precision moldingInformation Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 7.20 µm/m-°C @Temperature 20.0 - 300 °C |
4.00 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott NG9 Neutral Density Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include NG3, NG4, NG5, NG1, NG10, NG11, NG 12 |
|||
CTE, linear | 7.20 µm/m-°C @Temperature -30.0 - 70.0 °C |
4.00 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-BAF4 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 7.20 µm/m-°C @Temperature 25.0 - 700 °C |
4.00 µin/in-°F @Temperature 77.0 - 1290 °F |
|
CeramTec 771 94% Alumina (Al2O3) Te value is 840°C. Hasselman Thermal Shock value is 200 K.Data provided by CeramTec North America. |
|||
CTE, linear | 7.20 µm/m-°C @Temperature 25.0 - 500 °C |
4.00 µin/in-°F @Temperature 77.0 - 932 °F |
ASTM-C372 |
CoorsTek ADS-96R 96% Alumina Thick Film Substrate This high-purity material ensures strong, reliable performance for ceramic substrate application. Applications: thick films and lasers |
|||
CTE, linear | 7.20 µm/m-°C @Temperature 25.0 - 500 °C |
4.00 µin/in-°F @Temperature 77.0 - 932 °F |
ASTM-C372 |
CoorsTek ADS-995R MidFilm™ 99.5% Alumina Thick Film Applications: thick films and lasers |
|||
CTE, linear | 7.20 µm/m-°C @Temperature 25.0 - 500 °C |
4.00 µin/in-°F @Temperature 77.0 - 932 °F |
ASTM-C372 |
CoorsTek ADSR-96R DuraStrate™ 96% Alumina Thick Film Applications: thick films and lasers |
|||
CTE, linear | 7.20 µm/m-°C @Temperature 25.0 - 600 °C |
4.00 µin/in-°F @Temperature 77.0 - 1110 °F |
ASTM-C372 |
CoorsTek Superstrate® 996 99.6% Alumina Thin Film Applications: thin film substrates |
|||
CTE, linear | 7.20 µm/m-°C @Temperature 25.0 - 600 °C |
4.00 µin/in-°F @Temperature 77.0 - 1110 °F |
ASTM-C372 |
CoorsTek Superstrate® TPS 99.6% Alumina Thin Film Applications: thin film substrates |
|||
CTE, linear | 7.20 µm/m-°C @Temperature 30.0 - 150 °C |
4.00 µin/in-°F @Temperature 86.0 - 302 °F |
|
Ametek Molybdenum-Copper Composite AMC 8020 Information supplied by Ametek Specialty Metal Products.The material is available as finished parts with the following maximum dimensions:Width: 6 inches (152 mm)Thickness: 0.150 inches (3.8 mm)Leng.. |
|||
CTE, linear | 7.20 µm/m-°C @Temperature 538 °C |
4.00 µin/in-°F @Temperature 1000 °F |
|
ATI Wah Chang Nb/Nb Alloy C-103 This alloy satisfies most rocket engine applications for temperatures up to 2700°F because of superior mechanical properties at all temperatures. Offers weight savings over many rocket engine desig.. |
|||
CTE, linear | 7.20 µm/m-°C @Temperature 20.0 - 400 °C |
4.00 µin/in-°F @Temperature 68.0 - 752 °F |
DIN EN 821-1 |
CeramTec B 40 Alumina, 99.1% B 40 is the ideal sliding mate with the same properties as Rubalit® A 1896. It contains a larger share of Al2O3 for superior chemical stability. |
|||
CTE, linear | 7.20 µm/m-°C @Temperature 20.0 - 400 °C |
4.00 µin/in-°F @Temperature 68.0 - 752 °F |
DIN EN 821-1 |
CeramTec Rubalit® IS 95 Brown Alumina Rubalit® IS 95 brown is a high-performance alumina ceramic. Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at.. |