Material Notes:
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include BC20
Physical Properties Metric English Comments
Density 3.62 g/cc
0.131 lb/in³
Thermal Properties Metric English Comments
CTE, linear 6.10 µm/m-°C

@Temperature -30.0 - 70.0 °C
3.39 µin/in-°F

@Temperature -22.0 - 158 °F
7.20 µm/m-°C

@Temperature 20.0 - 300 °C
4.00 µin/in-°F

@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 660 °C
1220 °F
Optical Properties Metric English Comments
Refractive Index 1.69

@Wavelength 587.6 nm
1.69

@Wavelength 587.6 nm
He
Transmission, Visible 88 %

@Wavelength 653 nm
88 %

@Wavelength 653 nm
Internal transmittance of 100% at 653 nm.
IR Transmittance 88 %

@Wavelength 1100 - 1200 nm
88 %

@Wavelength 1100 - 1200 nm
Internal transmittance of 99-100%  from 1100-1250 nm.
UV Transmittance <= 6.0 %

@Wavelength 200 - 291 nm
<= 6.0 %

@Wavelength 200 - 291 nm
82 %

@Wavelength 399 nm
82 %

@Wavelength 399 nm
Internal transmittance of 93% at 399 nm
Reflection Coefficient, Visible (0-1) 0.88
0.88
Chemical Properties Metric English Comments
Acid Class, SR 52.2
52.2
Alkali Class, AR 1.2
1.2
Stain Resistance Class, FR 1
1
Users viewing this material also viewed the following: