Material Notes:
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include NG3, NG4, NG5, NG1, NG10, NG11, NG 12
Physical Properties Metric English Comments
Density 2.44 g/cc
0.0882 lb/in³
Thermal Properties Metric English Comments
CTE, linear 6.40 µm/m-°C

@Temperature -30.0 - 70.0 °C
3.56 µin/in-°F

@Temperature -22.0 - 158 °F
7.20 µm/m-°C

@Temperature 20.0 - 300 °C
4.00 µin/in-°F

@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 487 °C
909 °F
Optical Properties Metric English Comments
Refractive Index 1.51

@Wavelength 587.6 nm
1.51

@Wavelength 587.6 nm
He
Transmission, Visible 3.0 - 6.0 %

@Wavelength 410 - 690 nm
3.0 - 6.0 %

@Wavelength 410 - 690 nm
8.0 %

@Wavelength 700 nm
8.0 %

@Wavelength 700 nm
Internal transmittance of 9%  at 700 nm
IR Transmittance 49 %

@Wavelength 2600 nm
49 %

@Wavelength 2600 nm
Internal transmittance of 53% at 2600 nm.
UV Transmittance <= 1.0 %

@Wavelength 200 - 390 nm
<= 1.0 %

@Wavelength 200 - 390 nm
Internal transmittance of 0.001% from 200-390 nm.
Reflection Coefficient, Visible (0-1) 0.92
0.92
Chemical Properties Metric English Comments
Acid Class, SR 3.2
3.2
Alkali Class, AR 2
2
Stain Resistance Class, FR 1
1