Schott NG10 Neutral Density Filter

Category Ceramic , Glass , Filter , Optical
Manufacturer Schott Glas Mainz
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Schott NG10 Neutral Density Filter.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include NG3, NG4, NG5, NG9, NG1, NG11, NG 12
Physical Properties Metric English Comments
Density 2.47 g/cc
0.0892 lb/in³
Thermal Properties Metric English Comments
CTE, linear 6.40 µm/m-°C

@Temperature -30.0 - 70.0 °C
3.56 µin/in-°F

@Temperature -22.0 - 158 °F
7.20 µm/m-°C

@Temperature 20.0 - 300 °C
4.00 µin/in-°F

@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 468 °C
874 °F
Optical Properties Metric English Comments
Refractive Index 1.52

@Wavelength 587.6 nm
1.52

@Wavelength 587.6 nm
He
Transmission, Visible 1.0 %

@Wavelength 680 - 700 nm
1.0 %

@Wavelength 680 - 700 nm
2.0 %

@Wavelength 700 nm
2.0 %

@Wavelength 700 nm
Internal transmittance
IR Transmittance 37 %

@Wavelength 2600 nm
37 %

@Wavelength 2600 nm
Internal transmittance of 40% at 2600 nm.
UV Transmittance <= 0.060 %

@Wavelength 200 - 390 nm
<= 0.060 %

@Wavelength 200 - 390 nm
Internal transmittance of 0.001% from 200-390 nm.
Reflection Coefficient, Visible (0-1) 0.92
0.92
Chemical Properties Metric English Comments
Acid Class, SR 3.2
3.2
Alkali Class, AR 2
2
Stain Resistance Class, FR 1
1