Thermal Properties Metric English Comments
CTE, linear 6.30 µm/m-°C

@Temperature 20.0 - 450 °C
3.50 µin/in-°F

@Temperature 68.0 - 842 °F
H.C. Starck HPM 1700 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
CTE, linear 6.30 µm/m-°C

@Temperature 20.0 - 100 °C
3.50 µin/in-°F

@Temperature 68.0 - 212 °F
H.C. Starck HPM 1710 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
CTE, linear 6.30 µm/m-°C

@Temperature 20.0 - 100 °C
3.50 µin/in-°F

@Temperature 68.0 - 212 °F
H.C. Starck MoCu 80/20 Molybdenum-Copper Composite Material
Description of Product: Molybdenum-copper composite materials are produced by copper infiltration of porous sintered molybdenum. They are available with different copper contents (15 - 35 %). A t..
CTE, linear 6.30 µm/m-°C

@Temperature 20.0 - 300 °C
3.50 µin/in-°F

@Temperature 68.0 - 572 °F
H.C. Starck MoCu 85/15 Molybdenum-Copper Composite Material
Description of Product: Molybdenum-copper composite materials are produced by copper infiltration of porous sintered molybdenum. They are available with different copper contents (15 - 35 %). A t..
CTE, linear 6.30 µm/m-°C

@Temperature -30.0 - 70.0 °C
3.50 µin/in-°F

@Temperature -22.0 - 158 °F
Schott N-SK16 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 6.30 µm/m-°C

@Temperature 20.0 - 300 °C
3.50 µin/in-°F

@Temperature 68.0 - 572 °F
Schott KG2 Short Pass Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include KG1, KG3, KG4, KG5
CTE, linear 6.30 µm/m-°C

@Temperature 20.0 - 300 °C
3.50 µin/in-°F

@Temperature 68.0 - 572 °F
ASTM-C372
CeramTec Rubalit® 708 Alumina, 96%
Based on 96% aluminum oxide, Rubalit® 708 was developed specifically for making heavy-duty resistors and miniature metal layer resistors. Because of its outstanding strength, this same material is ..
CTE, linear 6.30 µm/m-°C

@Temperature 25.0 - 300 °C
3.50 µin/in-°F

@Temperature 77.0 - 572 °F
ASTM-C372
CoorsTek Superstrate® TPS 99.6% Alumina Thin Film
Applications: thin film substrates
CTE, linear 6.30 µm/m-°C

@Temperature 149 °C
3.50 µin/in-°F

@Temperature 300 °F
ATI Wah Chang Zircadyne® Alloy Zr 702
Zircadyne 702 is commercially pure zirconium. Alloy exhibits good ductility even at cryogenic temperatures and good strength comparable with other common engineering alloys.Information provided by A..
CTE, linear 6.30 µm/m-°C

@Temperature -30.0 - 70.0 °C
3.50 µin/in-°F

@Temperature -22.0 - 158 °F
Schott N-LAK9 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 6.30 µm/m-°C

@Temperature 20.0 - 400 °C
3.50 µin/in-°F

@Temperature 68.0 - 752 °F
hardened to 62 HRC
Bohler-Uddeholm O1 Cold Work Tool Steel
Manganese-chromium-tungsten alloyed steelA general purpose oil hardening tool steel suitable for back up and punch holder plates. Features of this grade include a good combination of high surface ha..